Comparative evaluation of collagen and amniotic membrane scaffolds biofunctionalized with Wharton's jelly stem cell-conditioned medium and zinc oxide nanoparticles for gingival fibroblast metabolic activity and attachment.
Mohammadreza Karimi, Hengameh Dortaj, Zahra Moradi, Parsa Vafaei, Artak Heboyan, Seyed Ali Mosaddad, Farin Kiany
Oral and Dental Diseases Research Center, School of Dentistry, Shiraz University of Medical Sciences, Shiraz, Iran. · Tissue Engineering Research Group, Department of Anatomy and Cell Biology, Mashhad University of Medical Sciences, Mashhad, Iran.
Key points
From the paper's conclusion- AM-ZnO-NPs + CM showed the highest mean metabolic activity under the tested conditions. These descriptive findings support further investigation but do not establish synergy, superior adhesion, or periodontal regenerative efficacy.
Abstract
AIM: This in vitro study compared gingival fibroblast responses to collagen and amniotic membrane (AM) scaffolds, with zinc oxide nanoparticles (ZnO-NPs) and Wharton's jelly mesenchymal stem cell-conditioned medium (WJMSCs-CM). MATERIALS AND METHODS: Fibroblasts derived from three donors were cultured on collagen, AM, or AM-ZnO-NPs, with or without WJMSCs-CM. Metabolic activity was assessed using the tetrazolium reduction assay (MTT) at 48 and 72 h. Nuclear distribution was examined qualitatively using 4',6-diamidino-2-phenylindole (DAPI) staining, and cell-scaffold morphology using field emission scanning electron microscopy (FESEM). Energy-dispersive X-ray analysis assessed elemental composition. Group means and standard deviations were summarized descriptively; conditioned-medium contrasts and the ZnO-by-conditioned-medium contrast within AM were calculated without inferential testing. RESULTS: Mean relative MTT signals were higher at 72 h than at 48 h in every group. AM-ZnO-NPs + CM had the highest mean signals: 134.3 ± 12.76% at 48 h and 196.4 ± 4.15% at 72 h. At 72 h, AM, AM-ZnO-NPs, collagen, AM + CM, and collagen + CM yielded 150.3 ± 14.48%, 175.2 ± 9.82%, 144.0 ± 17.47%, 159.8 ± 13.90%, and 150.2 ± 13.54%, respectively. DAPI and FESEM images illustrated nuclear distribution and cell-associated surface morphology, without quantitative proliferation or adhesion measurements. CONCLUSION: AM-ZnO-NPs + CM showed the highest mean metabolic activity under the tested conditions. These descriptive findings support further investigation but do not establish synergy, superior adhesion, or periodontal regenerative efficacy.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Enhancement of osteogenic differentiation in umbilical cord mesenchymal stem cells using a silver nanoparticle-embedded carboxymethyl cellulose nano scaffold.Journal of applied oral science : revista FOB · 2026
- Development of zein-coated Ag-NPs integrated into decellularized fish skin extracellular matrix as a hybrid scaffold for wound healing: In-vitro and in vivo study.Injury · 2026
- Synthesis, Characterization, and Multifunctional Applications of Chitosan-Grafted-Poly(Acrylic Acid-Co-Acrylamide)/ZnO Nanocomposite Hydrogel: Loading Studies, Antimicrobial Activity, Wound Healing, and Anticancer Potential.International journal of nanomedicine · 2026
- Immune regulative GelMA&Zn2+/Ce3+-whitlockite scaffolds with continuous ions release for bone regenerationBioactive Materials · 2025
- In vitro culture of bovine ovarian cortex fragments supplemented with magnesium-doped zinc oxide nanocomposites.Reproductive biology · 2026
- Antibacterial and cell-instructive chitosan/NeoNectin hydrogels crosslinked via click chemistry enable osteogenic differentiation within ultra-soft matricesCarbohydrate Polymers · 2026