Journal of the mechanical behavior of biomedical materials

Mechanical behaviour of formable bioactive glass composite bone tissue scaffolds using a silica gel binder.

Marzieh Matinfar, Anastasia Elias, John A Nychka

Department of Chemical and Materials Engineering, University of Alberta, Edmonton, Alberta, T6G 1H9, Canada. Electronic address: matinfar@ualberta.ca. · Department of Chemical and Materials Engineering, University of Alberta, Edmonton, Alberta, T6G 1H9, Canada.

Key points

From the paper's conclusion
  • Here, we investigated 45S5 bioactive glass composite scaffolds in which glass particles were bonded by silica gel binders with systematically varied pH, silica concentration, and binder content.

Abstract

Waterglass-derived silica hydrogels are promising binders for formable, in situ-setting bone scaffolds, with acid-initiated formulations previously shown to gel within a clinically relevant timeframe (∼10 min). Here, we investigated 45S5 bioactive glass composite scaffolds in which glass particles were bonded by silica gel binders with systematically varied pH, silica concentration, and binder content. Compressive strength was highly composition-dependent, ranging from 14 kPa for composites prepared with the least concentrated basic gel at lower binder content to 625 kPa for those prepared with the most concentrated acidic gel at higher binder content. Although strength generally followed the corresponding pure-gel trends, strengthening after bioactive glass incorporation varied from ∼1.2-fold to >10-fold in the weakest and strongest systems, respectively, indicating that performance depended on both gel properties and particle-binder interactions. Microstructural analysis showed that the gel acted primarily as particle coatings and interparticle bridges rather than as a continuous matrix; higher binder content produced more extensive gel coverage and more continuous particle bonding. All composites exhibited nonlinear stress-strain behaviour characteristic of bonded granular materials, with limited strain at maximum stress (∼0.01-0.09). Most formulations showed negligible time-dependent strengthening compared with pure gels, consistent with accelerated aging of the confined gel phase within thin coatings and bridges. Failure analysis revealed a transition from barreling and mixed-mode cracking in weaker, more deformable systems to localized shear or axial splitting in stronger, more constrained systems. These findings establish processing-microstructure-property relationships for tuning formable, in situ setting bioactive glass scaffolds.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Mechanical behaviour of formable bioactive glass composite bone tissue scaffolds using a silica gel binder — Science Skim