Staircase block-cycling compression of hierarchically porous DIW titanium scaffolds: Effect of low-temperature gas nitriding.
K Slámečka, C Oliver-Urrutia, L Drotárová, A Kashimbetova, M Remešová, S Tkachenko, P Gejdoš, L Čelko,
Central European Institute of Technology, Brno University of Technology, Purkyňova 123, Brno, 612 00, Czechia; Faculty of Mechanical Engineering, Brno University of Technology, Technická 2, Brno, 616 69, Czechia; Institute of Physics of Materials CAS, v. v. i., Czech Academy of Sciences, Žižkova 22, Brno, 616 00, Czechia. Electronic address: karel.slamecka@ceitec.vutbr.cz. · Central European Institute of Technology, Brno University of Technology, Purkyňova 123, Brno, 612 00, Czechia.
Key points
From the paper's conclusion- This study investigates the cyclic behaviour of as-sintered and low-temperature gas-nitrided (500 °C and 600 °C for 10 h) direct ink writing titanium scaffolds with open-microporous struts under staircase block-cycling compression.
Abstract
This study investigates the cyclic behaviour of as-sintered and low-temperature gas-nitrided (500 °C and 600 °C for 10 h) direct ink writing titanium scaffolds with open-microporous struts under staircase block-cycling compression. Staircase block-cycling served as an accelerated testing protocol to analyse the evolution of ratcheting, stiffness, energy dissipation, torsional response, and transient cycle-to-cycle events over progressively increasing load levels. The cyclic response was characterised by an early stage governed by contact stabilisation and a later stage dominated by deformation localised within shear bands. Nitriding did not change the scaffold-scale failure mode, and cycles to failure remained similar among the three groups. Nevertheless, nitriding changed the cyclic deformation response. The 500 °C treatment showed the lowest observed mean pre-yield ratcheting, while the 600 °C treatment provided stronger resistance to later-stage irreversible deformation, reflected by slower ratcheting accumulation together with low loss factor and residual torque. Analysis of torsional signals and transient events further showed that nitriding influenced load redistribution and increased event severity. These findings indicate that low-temperature nitriding can be used to tailor cyclic deformation behaviour in architected microporous titanium scaffolds.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fracture resistance of zirconia fixed dental prostheses after low-temperature degradation and/or cyclic fatigue.Journal of prosthodontics : official journal of the American College of Prosthodontists · 2026
- 3D-printing for zirconia abutment manufacturing and screw access hole effect: fatigue behavior of milled zirconia simplified restorations.Odontology · 2026
- Cyclic deformation behavior and fatigue life prediction of 316H stainless steel under strain-controlled fatigueJournal of Materials Research and Technology · 2026
- Computational Performance Evaluation of Porous Ti-6Al-4V Scaffold Architectures for Femoral Defect Healing Using a Coupled Finite Element-Mechanoregulation Framework.Journal of biomedical materials research. Part B, Applied biomaterials · 2026
- Cyclic Stress Loading Induced Degradation of Silicon Nitride Ceramics Evaluated by Microcantilever Bending TestsJournal of the American Ceramic Society · 2026
- Nonlinear Fatigue Mechanical Behavior and Damage Evolution of Salt Rock Under Stepwise Cyclic Loading: Insight from Strain-Driven PerspectiveApplied Sciences · 2026