Journal of hazardous materials

Mechanism of in-situ calcium sulfate in the synergistic sulfidation-carbothermal reduction for efficient recovery of Cu, Pb, and Zn from copper smelting flue coated materials.

Kai Fan, Haipei Zhang, Bo Li, Shichao Wu, Yonggang Wei, Hua Wang

Faculty of Metallurgical and Energy Engineering, Kunming University of Science and Technology, Kunming 650093, China; State Key Laboratory of Complex Nonferrous Metal Resources Clean Utilization, Kunming University of Science and Technology, Kunming 650093, China. · Faculty of Metallurgical and Energy Engineering, Kunming University of Science and Technology, Kunming 650093, China; State Key Laboratory of Complex Nonferrous Metal Resources Clean Utilization, Kunming University of Science and Technology, Kunming 650093, China. Electronic address: 20230115@kust.edu.cn.

Key points

From the paper's conclusion
  • Flue coated materials from copper smelting are hazardous wastes rich in Cu, Pb, and Zn, containing intrinsic CaSO4.

Abstract

Flue coated materials from copper smelting are hazardous wastes rich in Cu, Pb, and Zn, containing intrinsic CaSO4. Unlike processes relying mainly on externally added sulfur sources, this study evaluates whether intrinsic CaSO4 can serve as an in-situ sulfur donor and slag-forming flux during sulfidation-carbothermal reduction. Thermodynamic calculations, in-situ XRD, and TG-MS were combined to investigate phase evolution and metal partitioning. CaSO4 remained stable below about 900 ℃, was reduced to CaS mainly at 900-1050 °C, and participated in CaO formation and SO2 release above about 1050 °C. Significant CO, CO2, SO2 release occurred above 1000 ℃, defining a reaction-active window of 1050-1200 °C. The CaSO4/C ratio strongly influenced oxygen-sulfur potential. insufficient carbon left CaSO4 undecomposed, an appropriate ratio favored Cu2S and FeS, and excess carbon promoted metallic alloying. The overall mechanism is supplying sulfur at low T, making slag at high T, and regulating oxygen-sulfur potential in the middle stage, which enables selective separation and recycling of Cu from Pb and Zn into matte and volatile phases, with efficiencies of 95.1 ± 0.9%, 92.2 ± 1.1%, and 90.1 ± 1.3%. The volatile Pb/Zn species and SO2 generated require downstream capture and off-gas treatment, but the capture efficiency was not evaluated in this study.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers