Investigations on the delamination mechanism of double-glass photovoltaic modules based on laser treating.
Chang Xiao, Shaojie Fu, Li Meng, Beibei Zhu, Wenchang Xie, Ruifeng Luo, Kaiwen Wei, Li Niu,
Wuhan National Laboratory for Optoelectronics, Huazhong University of Science and Technology, Wuhan, 430074, China. · Research Institute of Energy Science and Technology, State Power Investment Corporation, Shanghai, 200240, China; School of Water Resources and Hydropower Engineering, Xi'an University of Technology, Xi'an, 710048, China. Electronic address: fu.shaojie1@163.com.
Key points
From the paper's conclusion- Four characteristic states emerged with increasing laser energy density: non-separable, difficult-to-delaminate, stable delamination, and carbonized delamination.
Abstract
The growing number of decommissioned photovoltaic (PV) modules calls for efficient recycling methods with minimal material damage. This study developed a preheating-assisted pulsed laser strategy for interfacial delamination of double-glass crystalline silicon PV modules and investigated the underlying mechanisms. Preheating softened the EVA encapsulant and broadened the laser-processing window, although preheating alone was insufficient to induce EVA/Si delamination. Among the investigated conditions, a heater setpoint of 200 °C provided the widest stable-delamination window. The laser beam passed through the top glass and upper EVA encapsulant with limited optical loss and was predominantly absorbed by silicon. Four characteristic states emerged with increasing laser energy density: non-separable, difficult-to-delaminate, stable delamination, and carbonized delamination. Interfacial weakening involved coupled responses of EVA, the SiNx antireflection layer, and the silicon surface. EVA deacetylation reduced the abundance of polar ester groups and weakened chemical adhesion, while damage to the SiNx layer and localized silicon melting-resolidification altered the interfacial bonding environment and reduced mechanical interlocking. Transient pressure from localized vaporization and volatile-product release may have further assisted crack propagation across regions where the pyramidal texture remained intact. These coupled effects enabled relatively continuous EVA/Si delamination with limited material damage. Excessive energy input caused EVA carbonization, severe surface ablation, and silicon fracture. These findings provide a mechanistic basis for process optimization and low-damage recovery of materials from double-glass PV modules.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Laser‐Assisted Delamination for High‐Value Recycling of Solar PanelsProgress in Photovoltaics Research and Applications · 2025
- Process Regime Mapping of Green Picosecond Laser Delamination Through Glass in POE Photovoltaic Laminates After Field AgingApplied Sciences · 2026
- Laser-induced delamination of aged silicon photovoltaic modules to achieve >95% selective silver recoveryCommunications Materials · 2026
- Solvent‐Based Chemical Delamination of End‐Of‐Life Photovoltaic Modules: A Systematic ReviewSolar RRL · 2026
- Strength and Stiffness of Double-Glass (3.2 mm) PV Panels Laminated with Soft Siloxane (PDMS) Gel for Zero Emission Room-Temperature Intact-Glass Recycling: Comparison with Double-Glass (1.6 mm) PV Panels Laminated with Solid EVA PolymerSustainability · 2026
- Effect of Temperature on the Glass Delamination in End-of-Life of Crystalline Silicon Photovoltaic PanelsGreen · 2026