Sulfur-vacancy-mediated dynamic self-stabilization of nickel sulfide/Oxyhydroxide Heterostructures for durable alkaline hydrogen evolution.
Zhenzhen Yang, Jialun Liu, Xuye Cao, Yatai Li, Jianhui Xie, Genlei Zhang, Luofu Min, Peng Cui
Anhui Province Key Laboratory of Value-Added Catalytic Conversion and Reaction Engineering, School of Chemistry and Chemical Engineering, Hefei University of Technology, Hefei 230009, PR China. · Anhui Province Key Laboratory of Value-Added Catalytic Conversion and Reaction Engineering, School of Chemistry and Chemical Engineering, Hefei University of Technology, Hefei 230009, PR China. Electronic address: genleizhang@hfut.edu.cn.
Key points
From the paper's conclusion- These results indicate that implanted VS initiate a dynamic surface reconfiguration cycle, in which OH- adsorption and activation promote continuous formation of fresh Ni3S2/NiOOH interfaces, compensating activity decay.
Abstract
Alkaline water electrolysis requires non-precious hydrogen evolution reaction (HER) catalysts with high activity and durability. We report a two-step strategy combining hydrothermal sulfidation and electrochemical reductive etching to construct a sulfur-vacancy-rich Ni3S2/NiOOH heterostructure on nickel foam (Ni3S2/NiOOH-VS/NF). The etching simultaneously generates abundant sulfur vacancy (VS) and induces in situ NiOOH reconstruction. The catalyst exhibits excellent HER activity in 30 wt% KOH at 80 °C, requiring only 85.6 mV overpotential at 10 mA cm-2 and a Tafel slope of 83.4 mV dec-1. It operates stably for 1000 h at 100 mA cm-2 with a potential increase of only 22.1 mV, maintains stable activity for 500 h at a constant overpotential of 185 mV, and exhibits only 7 mV decay after 100 start/stop cycles, superior to NF and Ni3S2/NF. Post-test characterizations reveal that the Ni3S2 framework is preserved, while S slowly leaches, VS are partially refilled, and NiOOH is enriched. These results indicate that implanted VS initiate a dynamic surface reconfiguration cycle, in which OH- adsorption and activation promote continuous formation of fresh Ni3S2/NiOOH interfaces, compensating activity decay. This defect-mediated self-stabilizing mechanism provides a practical route to durable non-precious HER catalysts for alkaline water electrolysis.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Surface Hydroxylation‐Engineered Ni₃ S₂ /Ni‐OH Heterostructure for Durable Alkaline Hydrogen Evolution via Facile pH‐Induced ElectrodepositionAdvanced Functional Materials · 2025
- Sulfur leaching-triggered reconstruction of sulfurized nickel molybdate toward ampere-level alkaline hydrogen evolution reaction.Journal of colloid and interface science · 2026
- Sulfur Vacancy-Engineered Co9S8-Ni3S4 Heterostructure as a Hydrogen Spillover Catalyst for Efficient Alkaline Water Splitting.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2025
- Structural and Electrochemical Evolution of Nickel Sulfides During Alkaline Hydrogen Evolution ReactionChemSusChem · 2025
- Fe-Regulated Sulfidation of Ni-MOF to Construct an Fe-Ni(OH)2/Ni3S2 Heterojunction for Efficient Hydrogen Evolution in Both Acidic and Alkaline Media.ACS applied materials & interfaces · 2026
- Preconfiguring a High−Valent Ni State Decouples Lattice−Oxygen Activation From Dynamic Surface Reconstruction for Stable Water Oxidation at 2.0 A cm−²Advanced Energy Materials · 2026