Enhanced phosphoric acid retention and durability of high-temperature proton exchange membrane fuel cells with zeolite-modified cathode catalyst layers.
Hongxiang Zheng, Feng Huang, Gui Ren, Junwen Deng, Xinhai Yu, Shan-Tung Tu
Key Laboratory of Pressure Systems and Safety (MOE), School of Mechanical and Power Engineering, East China University of Science and Technology, Shanghai 200237, China. · Key Laboratory of Pressure Systems and Safety (MOE), School of Mechanical and Power Engineering, East China University of Science and Technology, Shanghai 200237, China. Electronic address: yxhh@ecust.edu.cn.
Key points
From the paper's conclusion- Overall, the experimental findings demonstrate improved whole-MEA PA retention and long-term stability through zeolite modification, while the simulations provide a possible molecular-level interpretation of these improvements.
Abstract
High-temperature proton exchange membrane fuel cells (HT-PEMFCs) suffer from phosphoric acid (PA) loss and catalyst layer (CL) degradation during prolonged operation, which limits their durability. In this study, NaY zeolite was incorporated into the cathode CL to improve PA retention and operational stability. Its effects were investigated using durability testing, acid-base titration, electrochemical impedance spectroscopy (EIS), transmission electron microscopy (TEM), and molecular dynamics (MD) simulations. Under methanol reformate/air at 0.2 A cm-2, the modified membrane electrode assembly (MEA) retained 98.7% of its stabilized voltage after 1400 h, whereas the conventional MEA retained 80.4% after 1000 h, when the test was terminated because of pronounced performance degradation. At their respective end of test (EOT) states, the modified MEA and conventional MEA retained 81.7% and 53.6% of their initial PA contents, respectively. The modified MEA also exhibited smaller increases in charge transfer resistance and mass transport resistance and less pronounced Pt particle growth. MD simulations showed that zeolite incorporation increased the population of PA molecules associated with Na-containing sites while decreasing the simulated free-PA and Ptsurface-near fractions. Within the zeolite-containing CL model, Na-associated PA states exhibited more persistent residence characteristics than the Ptsurface-near states. These results suggest that zeolite-associated environments may transiently accommodate PA and influence its local distribution. Overall, the experimental findings demonstrate improved whole-MEA PA retention and long-term stability through zeolite modification, while the simulations provide a possible molecular-level interpretation of these improvements.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Electrostatic Repulsion Activates Durable Pt Catalysts for HT‐PEMFCsAdvanced Energy Materials · 2026
- Binder Engineering for Phosphoric Acid Distribution and Retention in High-Temperature Proton Exchange Membrane Fuel Cell Cathodes.Advanced materials (Deerfield Beach, Fla.) · 2026
- Enhanced PEMFC Performance and Durability Enabled by a Highly Oxygen-Permeable Ionomer BinderACS Omega · 2026
- Cross-linked Ion-Pair Microporous Polymers Enabling Durable High-Temperature Proton Exchange Membrane Fuel Cells.Advanced materials (Deerfield Beach, Fla.) · 2026
- Topology Engineered Fluorinated Ionomers Alleviate the Trade‐off Between Oxygen Accessibility and Proton Transport in Low‐Pt HT‐PEMFC Catalyst LayersAdvanced Functional Materials · 2026
- Dual-Bond-Reinforced 3D Network Membrane with Nitrogen-Ratched Ionic Polymer for Enhanced Durability and High-Power HT-PEMFCs.ACS applied materials & interfaces · 2026