Journal of colloid and interface science

Water-limited shielding and zincophilic guiding of Zn(002) deposition for aqueous zinc-ion batteries.

Xiaomeng Guo, Bo Qin, Xiaotian Feng, Ming Li, Jingran Zhou, Zemin Feng, Zekun Zhang

School of Chemical Engineering, North China University of Science and Technology, Tangshan 063210, Hebei, China. · Yanzhao Iron and Steel Laboratory, North China University of Science and Technology, Tangshan, Hebei, 063210, China.

Key points

From the paper's conclusion
  • The study uses ultra-thin aramid nanofiber (Kevlar) coatings to construct a water-limited and zincophilic interface for aqueous zinc-ion batteries (AZIBs).
  • The Kevlar@Zn||Kevlar@Zn symmetric cell exhibited a cycle life exceeding 1360 h at a current density of 1 mA cm-2, and the Kevlar@Zn||MnO2 full cell retained 83.5% of its capacity after 350 cycles at a current density of 0.5 A g-1.
  • This work proposes a novel strategy for preparing artificial coatings that can advance the development of safe and stable zinc metal batteries.

Abstract

Aqueous zinc-ion batteries (AZIBs) have great potential for large-scale energy storage due to their high safety, excellent rate performance and cost-effectiveness. However, the industrial feasibility of the anode is fundamentally constrained by the sluggish Zn2+ transport at the interface and parasitic reactions with active water molecules, leading to uneven Zn deposition. Here, we report the use of ultra-thin aramid nanofiber (Kevlar) coatings to construct an water-limited and zincophilic interface. The hydrophobic main chain of Kevlar modulates the contact between the zinc metal and the aqueous environment, reducing interfacial active water to inhibit the hydrogen evolution reaction and corrosion. Simultaneously, the abundant polar amide groups in the Kevlar framework exhibit high affinity for Zn2+, promoting the desolvation of [Zn(H2O)6]2+ and guiding Zn2+ deposition along the (002) crystal plane. This synergistic regulation enables an ordered deposition/dissolution process under an ultrathin protective structure with a sub-micron thickness. Consequently, the Kevlar@Zn||Kevlar@Zn symmetric cell exhibited a cycle life exceeding 1360 h at a current density of 1 mA cm-2. Furthermore, the Kevlar@Zn||MnO2 full cell retained 83.5% of its capacity after 350 cycles at a current density of 0.5 A g-1. This work proposes a novel strategy for preparing artificial coatings, which can advance the development of safe and stable zinc metal batteries.

Read the paper

Discussion · 1

Science Skim's AI key points, plus readers' public thoughts

Science SkimAI key points
Pinned
  • The study uses ultra-thin aramid nanofiber (Kevlar) coatings to construct a water-limited and zincophilic interface for aqueous zinc-ion batteries (AZIBs).
  • The Kevlar@Zn||Kevlar@Zn symmetric cell exhibited a cycle life exceeding 1360 h at a current density of 1 mA cm-2, and the Kevlar@Zn||MnO2 full cell retained 83.5% of its capacity after 350 cycles at a current density of 0.5 A g-1.
  • This work proposes a novel strategy for preparing artificial coatings that can advance the development of safe and stable zinc metal batteries.