From monoanhydride to dianhydride: molecular engineering of electrolytes for chemomechanically stable NCM613||Si/C batteries.
Xinru Li, Changquan Wu, Yifan Wu, Du Liu, Xuerui Yang, Xiaowei Huang, Naigen Zhou
School of Physics and Materials Science, Nanchang University, 999 Xuefu Avenue, Nanchang 330031, China. · Jiujiang Tinci Materials Technology Co., Ltd., Jiujiang 332500, China.
Key points
From the paper's conclusion- High-energy LiNi0.6Co0.1Mn0.3O2 (NCM613) ||silicon/carbon (Si/C) full cells undergo pronounced interfacial chemomechanical degradation under high-voltage and high-temperature conditions, as repeated Si volume fluctuation, electrolyte decomposition, and transition-metal (TM) dissolution accelerate cell failure. Although monoanhydride additives such as succinic anhydride (SA) can scavenge acidic impurities, their limited reactive sites and insufficient structural adaptability restrict long-term interphase stabilization.
- 1,2,4,5-cyclohexanetetracarboxylic dianhydride (HPMDA) is introduced as a multifunctional electrolyte additive, extending additive design from monoanhydride to dianhydride.
- The coupled chemical-mechanical degradation is markedly suppressed, leading to improved cycling stability of NCM613||Si/C full cells, with capacity retentions of 80% after 400 cycles at 45 °C, 82% after 200 cycles at 55 °C, and 80% after 300 cycles at 4.6 V.
Abstract
High-energy LiNi0.6Co0.1Mn0.3O2 (NCM613) ||silicon/carbon (Si/C) full cells undergo pronounced interfacial chemomechanical degradation under high-voltage and high-temperature conditions, as repeated Si volume fluctuation, electrolyte decomposition, and transition-metal (TM) dissolution accelerate cell failure. Although monoanhydride additives such as succinic anhydride (SA) can scavenge acidic impurities, their limited reactive sites and insufficient structural adaptability restrict long-term interphase stabilization. To address these limitations, 1,2,4,5-cyclohexanetetracarboxylic dianhydride (HPMDA) is introduced as a multifunctional electrolyte additive, extending additive design from monoanhydride to dianhydride. Relative to SA, the dual-anhydride framework of HPMDA provides four carbonyl-active sites, enabling enhanced H2O/HF scavenging and more effective regulation of Li+ solvation, while the cyclohexane backbone imparts conformational flexibility for mechanically compliant interphases. HPMDA regulates the electrolyte solvation structure toward an aggregate-rich configuration and facilitates the preferential decomposition of fluoroethylene carbonate (FEC), thereby promoting the formation of thin and uniform solid electrolyte interphase (SEI) and cathode electrolyte interphase (CEI) layers that accommodate Si volume fluctuation and suppress cathode corrosion. Consequently, the coupled chemical-mechanical degradation is markedly suppressed, leading to improved cycling stability of NCM613||Si/C full cells, with capacity retentions of 80% after 400 cycles at 45 °C, 82% after 200 cycles at 55 °C, and 80% after 300 cycles at 4.6 V. These results reveal the structure-function relationship underlying the transition from monoanhydride to dianhydride additives and provide a molecular basis for electrolyte design that couples bulk chemistry, solvation structure, and interphase mechanics.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- High-energy LiNi0.6Co0.1Mn0.3O2 (NCM613) ||silicon/carbon (Si/C) full cells undergo pronounced interfacial chemomechanical degradation under high-voltage and high-temperature conditions, as repeated Si volume fluctuation, electrolyte decomposition, and transition-metal (TM) dissolution accelerate cell failure. Although monoanhydride additives such as succinic anhydride (SA) can scavenge acidic impurities, their limited reactive sites and insufficient structural adaptability restrict long-term interphase stabilization.
- 1,2,4,5-cyclohexanetetracarboxylic dianhydride (HPMDA) is introduced as a multifunctional electrolyte additive, extending additive design from monoanhydride to dianhydride.
- The coupled chemical-mechanical degradation is markedly suppressed, leading to improved cycling stability of NCM613||Si/C full cells, with capacity retentions of 80% after 400 cycles at 45 °C, 82% after 200 cycles at 55 °C, and 80% after 300 cycles at 4.6 V.
Readers' thoughts
No reader thoughts yet.
Related papers
- Ultra‐Stable High‐Voltage Cycling of Li‐Ion Batteries via Interphase Engineering with 3,5‐Bis(trifluoromethyl)phenyl IsocyanateAdvanced Functional Materials · 2026
- Self‐Organized Interfacial Engineering Enabling Stable SiO x –MgSiO 3 @C Anodes via Magnesiothermic ReductionJournal of the American Ceramic Society · 2026
- In Situ Assembled Carboxyl-Functionalized Hexaazatrinaphthylene Enables Accelerated Li+ Transport and Localized FEC Enrichment in Silicon Anodes.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Dual‐Ion Reconstruction of a LiF/NaF–N‐Rich Hybrid Interphase for Durable Silicon‐Carbon AnodesAdvanced Functional Materials · 2026
- Complementary Functional-Group Integration Directs Interphase Chemistry toward High-Temperature Stable Ni-Rich CathodesACS Sustainable Chemistry & Engineering · 2026
- Synergistic Carboxymethyl Cellulose-Phytic Acid Binders Enabling Exceptional Silicon AnodesIndustrial & Engineering Chemistry Research · 2026