From the paper's conclusion
  • When incorporated into epoxy (EP) coatings, hZIF-8 proposed to introduce an ångström-scale ion-trapping mechanism.

Abstract

Zeolitic imidazolate framework-8 (ZIF-8) holds great promise as a corrosion inhibitor carrier owing to its high specific surface area; however, its 3.4 Å aperture restricts the diffusion of inhibitors into the 11.6 Å cavities. Herein, ZIF-8 was etched into a hollow structure (hZIF-8) using tannic acid (TA), leading to phenolate-rich, hydrophilic functional shell and enlarged pore sizes. When incorporated into epoxy (EP) coatings, hZIF-8 proposed to introduce an ångström-scale ion-trapping mechanism. The hydrated radii of Cl − and Na + exceed the pore window, necessitating partial dehydration, which is followed by rehydration inside the confined cavity, and a second dehydration step to exit. This dehydration-rehydration loop, combined with electrostatic Cl − repulsion, partial Na + trapping, and ultra-tortuous diffusion pathways for ions within the cavities, enhances the corrosion resistance of EP coatings. Further grafting of benzotriazole onto hZIF-8 (BTA@hZIF-8) provides active inhibition properties while providing chloride trapping and/or barrier ability. Incorporation of the synthesized pigments into EP coatings resulted in high impedance at low frequency (|Z| 0.01 Hz ) of ~8 × 10 10 and ~ 10 11 Ω.cm 2 for hZIF-8/EP and BTA@hZIF-8/EP coatings after 245 days of immersion in salt media, which is two and three orders of magnitude higher than the blank EP coatings.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers