International journal of biological macromolecules

DMF-water cosolvation alters the apparent colloidal behavior of cellulose nanocrystals while retaining chiral nematic self-assembly.

Ruixin Liu, Tao Lin, Xuefeng Yin, Meng Yu, Yuxiang Wang, Jingtao Ren, Huide Zhang, Yunxing Tao,

College of Bioresources Chemical and Materials Engineering, Shaanxi University of Science and Technology, Shaanxi Provincial Key Laboratory of Papermaking Technology and Specialty Paper, National Demonstration Center for Experimental Light Chemical Engineering Education, Key Laboratory of Paper Based Functional Materials of China National Light Industry, Xi'an, 710021, Shaanxi, China. · College of Bioresources Chemical and Materials Engineering, Shaanxi University of Science and Technology, Shaanxi Provincial Key Laboratory of Papermaking Technology and Specialty Paper, National Demonstration Center for Experimental Light Chemical Engineering Education, Key Laboratory of Paper Based Functional Materials of China National Light Industry, Xi'an, 710021, Shaanxi, China. Electronic address: lintao@sust.edu.cn.

Key points

From the paper's conclusion
  • Overall, DMF-water cosolvation was associated with altered apparent colloidal and post-drying behavior while retaining cellulose I structure and chiral nematic self-assembly.

Abstract

Drying-induced association can hinder processing and rehydration of cellulose nanocrystals (CNCs). This study examined DMF-water cosolvation as a non-derivatizing approach to alter CNC colloidal behavior while preserving cellulose structure and chiral nematic self-assembly. CNC suspensions and the corresponding films were characterized using dynamic light scattering, ζ-potential analysis, atomic force microscopy, rheology, FTIR spectroscopy, and X-ray diffraction. At 2.2 wt% CNC, DMF shifted the modal apparent hydrodynamic diameter from approximately 80 to 55 nm and reduced the polydispersity index from 0.221 to 0.201, while ζ-potential changed slightly from -33.1 to -32.1 mV. Together with lower low-shear viscosity, these changes were consistent with altered apparent colloidal association rather than enhanced electrostatic stabilization; however, CNC-CNC interaction forces were not directly measured. FTIR indicated differences in the local vibrational environment, while XRD showed the retention of characteristic cellulose I reflections. CNC/DMF films retained birefringent textures, layered cross-sectional structures, and visible structural color after evaporation-induced self-assembly. After freeze-drying and rehydration, the DMF-treated sample showed less sedimentation and higher apparent dry-residue indices than the control. GC-MS measured residual DMF at 80.1 ± 0.6 mg L - 1 in the clarified liquid phase of the redispersed treated sample. Although the estimated direct mass contribution of detected DMF was smaller than the dry-residue-index difference, indirect effects of residual DMF and freeze-drying/rehydration could not be excluded. Overall, DMF-water cosolvation was associated with altered apparent colloidal and post-drying behavior while retaining cellulose I structure and chiral nematic self-assembly.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

DMF-water cosolvation alters the apparent colloidal behavior of cellulose nanocrystals while retaining chiral nematic self-assembly — Science Skim