International journal of biological macromolecules

Improving the antifouling performance of poly(lactic acid) membranes through the incorporation of cellulose nanocrystals.

Rana Memarzadeh, Vahid Vatanpour, Mohamadreza Nofar, Ismail Koyuncu

Polymer Science and Technology Department, Istanbul Technical University, Maslak, 34469, Istanbul, Türkiye. · Environmental Engineering Department, Istanbul Technical University, Maslak, 34469, Istanbul, Türkiye; Department of Applied Chemistry, Faculty of Chemistry, Kharazmi University, Tehran, 15719-14911, Iran. Electronic address: vahidvatanpour@khu.ac.ir.

Key points

From the paper's conclusion
  • To address the growing demand for sustainable water treatment and align with circular economy principles, this study investigates bio-based mixed-matrix nanocomposite membranes by incorporating cellulose nanocrystals (CNCs) into a poly(lactic acid) (PLA) matrix.

Abstract

To address the growing demand for sustainable water treatment and align with circular economy principles, this study investigates bio-based mixed-matrix nanocomposite membranes by incorporating cellulose nanocrystals (CNCs) into a poly(lactic acid) (PLA) matrix. CNCs were incorporated as hydrophilic nanofillers to improve the surface hydrophilicity and mechanical performance of PLA. PLA/CNC membranes were fabricated via nonsolvent-induced phase separation (NIPS) using dimethyl sulfoxide (DMSO) as a greener solvent, with CNC loadings varying from 0.1 to 2 wt%; 2 wt% (PLA/CNC2) was selected as the optimal threshold to avoid particle aggregation. Among the formulations investigated, PLA/CNC2 (2 wt% CNC) exhibited the most favorable overall performance. Characterization revealed changes in surface topography, an increase in porosity from 70.4% to 80.2%, and a decrease in water contact angle from 86.0° to 65.8°. The pure-water flux increased from 378.4 L·m-2·h-1 for pristine PLA to 490.2 L·m-2·h-1 for PLA/CNC2. During a five-hour sequential filtration test, PLA/CNC2 exhibited a higher flux recovery ratio (FRR) than pristine PLA (82.7% versus 55.0%) and a lower irreversible fouling ratio. The tensile strength of PLA/CNC2 reached 3.29 MPa, which, although modest for industrial-scale applications, is sufficient for low-pressure operation. Rejection rates reached 96.6% for BSA (500 mg·L-1), 83.2% for Reactive Black 5 (150 mg·L-1), and 91.6% for Reactive Red 120 (150 mg·L-1). The observed BSA rejection is consistent with size exclusion, whereas electrostatic interactions may contribute to the rejection of anionic dyes. These findings highlight the potential of CNC-modified PLA membranes for wastewater treatment applications.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers