International journal of biological macromolecules

Physical-chemical properties of TEMPO-oxidized nanocellulose/fucoidan composite structures.

Gabriela-Mădălina Oprică, Cătălina-Diana Uşurelu, Adriana Nicoleta Frone, Elena Iulia Neblea, Monica Florentina Raduly, Cristina Nistor, Cristian-Andi Nicolae, Anamaria Zaharia,

National Institute for Research and Development in Chemistry and Petrochemistry, 202 Splaiul Independentei, 060021, Bucharest, Romania; Faculty of Chemical Engineering and Biotechnology, National University of Science and Technology Politehnica Bucharest, 1-7 Gh. Polizu Street, 011061, Bucharest, Romania. · National Institute for Research and Development in Chemistry and Petrochemistry, 202 Splaiul Independentei, 060021, Bucharest, Romania. Electronic address: adriana.frone@icechim.ro.

Key points

From the paper's conclusion
  • Taking advantage of the water solubility and bioactivity of fucoidan, and the large surface area, good rheological properties, and nontoxicity of nanocellulose, in this work NC/F and TEMPO-oxidized-NC (NCT)/F composites with different proportions of the components (2/1, 1/1, and 1/2) were obtained and studied.

Abstract

Both fucoidan (F) and nanocellulose (NC) have attracted particular interest for use in pharmaceutical preparations and as a food additive, but their effects in NC/F composites remained underexplored. Taking advantage of the water solubility and bioactivity of fucoidan, and the large surface area, good rheological properties, and nontoxicity of nanocellulose, in this work NC/F and TEMPO-oxidized-NC (NCT)/F composites with different proportions of the components (2/1, 1/1, and 1/2) were obtained and studied. The morphological investigation of the composite structures by scanning electron microscopy revealed denser networks in the composites as compared to neat NC or NCT, while the structural investigation by Fourier-transform infrared spectroscopy confirmed the existence of physical interactions between NC or NCT and F, and the influence of F on the aggregation of nanofibers in the composites. The most important benefit resulting from mixing F with NC or NCT was observed from the analysis of their rheological properties. All the NC/F and NCT/F composites showed much higher apparent viscosity than F, regardless of the shear rate, the greatest increase in viscosity, almost 2500 times, being observed for NC/F21. The inverted tube test clearly showed the gelling capacity and good stability of the gels obtained from the NC/F mixtures and, especially, from the NCT/F mixtures. In the 24 h test, all NC and NC/F samples showed leaking when the tube was inverted, while the NCT and NCT/F gels remained stable. These composites with good rheological and thermal behaviors are suitable for future application in the cosmetics, pharmaceutical, and food industries.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers