One-step ball-milling toward tannin depolymerization and graphene exfoliation for rapid-curing and high-strength bio-based phenolic resins.
Zhiqin Wang, Hao Xie, Pu Liu, Yan Lyu, Xiaona Li, Jianzhang Li, Jiongjiong Li
Co-Innovation Center of Efficient Processing and Utilization of Forest Resources, College of Materials Science and Engineering, Nanjing Forestry University, Longpan Road 159, Xuanwu District, Nanjing, 210037, China. · College of Light Industry and Food Engineering, Nanjing Forestry University, Longpan Road 159, Xuanwu District, Nanjing, 210037, China.
Key points
From the paper's conclusion- The ball milling treatment reduced the polymerization degree of tannin from 7 to 1-2, thereby significantly reducing steric hindrance and enhancing reactivity, while ensuring the uniform dispersion of graphene nanosheets within the resin matrix.
Abstract
Traditional phenolic resins exhibit contradictions in biomass substitution, curing kinetics, and enhancements in mechanical properties, which severely restrict their applications in wood structural materials. To address these issues, this study proposes an integrated strategy that involves ball milling-mediated tannin depolymerization and graphene functionalization, resulting in the preparation of graphene-modified depolymerized tannin (DGAMT). The ball milling treatment reduced the polymerization degree of tannin from 7 to 1-2, thereby significantly reducing steric hindrance and enhancing reactivity, while ensuring the uniform dispersion of graphene nanosheets within the resin matrix. Phenol was partially substituted with DGAMT to prepare biomass-based phenolic resins (DGTCS), and chitosan oligomers were introduced to construct a robust hydrogen bond and high-density covalent crosslinking network. At a hot-pressing temperature of 120 °C, the optimal DGTCS-5 resin achieved a wet bonding strength of 1.62 MPa and a debonding work of 0.876 J; the latter was approximately twice that of the neat PF resin. The onset curing temperature decreased from 156.5 °C for the unmodified PF reference to 127.7 °C for DGTCS-5, and the gel time was markedly shortened. This strategy effectively addresses the challenges of biomass substitution, curing behaviors, and mechanical performance optimization, providing a novel technical pathway for the industrial development of high-performance biomass adhesives.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- High‐Performance Phenolic Resin Reinforced by Tannic Acid‐Polyethyleneimine Functionalized Multi‐Walled Carbon Nanotubes for Wood‐Based PanelsMacromolecular Rapid Communications · 2026
- Cell-wall mechanics in alkali-extracted and resin-impregnated densified birch wood by nanoindentationDiscover Materials · 2026
- Preparation and Characterization of Recyclable Basalt Fiber CompositesPolymer Composites · 2026
- Modification of Cork with Deep Eutectic Solvent and Dopamine for Enhanced Soy Protein-Based Wood AdhesivesACS Applied Engineering Materials · 2026
- Structure-property tailoring of acetone-fractionated Kraft lignin for high-performance phenol-resorcinol-formaldehyde structural adhesives.International journal of biological macromolecules · 2026
- Novel use of waste calcined clay brick powder in sustainable ultra-high ductility strain-hardening geopolymer composites: Micro-characteristics and mechanical behaviorApplied Clay Science · 2026