Electron-beam-crosslinked injectable poly-γ-glutamic acid hydrogels: Physicochemical properties, long-term in vivo retention, and biocompatibility.
Seo-Joon Yeom, Jeong Pyo Son, Minho Park, Beom-Seok Song, Jong-Heum Park, Yeung Bae Jin, Do-Yeong Kim, Jae-Kyung Kim
Advanced Radiation Technology Institute, Korea Atomic Energy Research Institute, Jeongeup, 56212, Republic of Korea; Department of Integrative Food, Bioscience and Biotechnology, Chonnam National University, Gwangju, 61186, Republic of Korea. · Advanced Radiation Technology Institute, Korea Atomic Energy Research Institute, Jeongeup, 56212, Republic of Korea.
Key points
From the paper's conclusion- Overall, EB irradiation enabled the preparation of injectable γ-PGA hydrogels with irradiation-dependent physicochemical and rheological properties, prolonged in vivo retention, practical injectability, and favorable biocompatibility.
Abstract
Injectable hydrogels for biomedical applications require controllable mechanical properties, sustained in vivo retention, and favorable biocompatibility. Here, injectable poly-γ-glutamic acid (γ-PGA) hydrogels were prepared by electron-beam (EB) irradiation at 30 kGy (low dose, LD), 150 kGy (medium dose, MD), and 200 kGy (high dose, HD), without additional chemical crosslinking agents. Nuclear magnetic resonance and Fourier-transform infrared analyses revealed irradiation-induced spectral changes in γ-PGA. Physicochemical and mechanical characterization demonstrated distinct differences in swelling behavior, gel fraction, rheological properties, and injection force among the irradiation groups. In vivo retention and biocompatibility were assessed in mice over 180 days following subcutaneous injection. Magnetic resonance imaging (MRI)-based volumetric analysis showed progressively prolonged retention from LD to HD, with γ-PGA (LD) remaining detectable through day 7, γ-PGA (MD) through day 150, and γ-PGA (HD) retaining 74.26 ± 3.77% of its initial volume on day 180. Higher irradiation levels were also associated with greater G' and G″ values and reduced maximum swelling. Compared with the hyaluronic acid hydrogel, the γ-PGA hydrogels exhibited less pronounced early post-injection volume expansion, while their long-term MRI-detectable volume profiles varied among the irradiation groups. No marked local or systemic adverse responses were detected based on MRI, histological observations, serum cytokine analysis, hematologic assessment, body weight monitoring, and relative organ weight measurements. Overall, EB irradiation enabled the preparation of injectable γ-PGA hydrogels with irradiation-dependent physicochemical and rheological properties, prolonged in vivo retention, practical injectability, and favorable biocompatibility.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Mechanistic insights on irradiation induced fabrication of nanoporous guar gum/chitosan pH responsive hydrogels: a combined DFT and spectroscopic study.RSC advances · 2026
- Biocompatible Gelatinized Starch as a Functional Modulator to Expand the Scope of Injectable Hydrogels.Advanced healthcare materials · 2026
- Durable Radiopaque Embolic Hydrogels via Iodinated Monomer Copolymerization for Transarterial ChemoembolizationJournal of Applied Polymer Science · 2026
- Gamma Radiation-Assisted Synthesis of Xanthan Gum/Acrylamide Hydrogels for Drug DeliveryGels · 2026
- Clinically Translatable Injectable Hydrogel Platform for Dual Intraoperative Elevation and Postoperative Healing in Endoscopic Submucosal DissectionACS Nano · 2025
- Radiation-Induced Synthesis of Crosslinker-Free Hydrogels via E-Beam: Structural Dynamics and Controlled Drug DeliveryInternational Journal of Molecular Sciences · 2026