Department of Polymer and Materials Chemistry, Faculty of Chemistry and Petroleum Sciences, Shahid Beheshti University, Tehran, Iran. · Department of Polymer and Materials Chemistry, Faculty of Chemistry and Petroleum Sciences, Shahid Beheshti University, Tehran, Iran. Electronic address: r_sedghi@sbu.ac.ir.
Key points
From the paper's conclusion- Together, these findings demonstrate that integrating macromolecule-mediated interfacial functionality with scaffold microporosity can support localized retention and staged delivery of cell-laden microcarriers for bone regeneration.
Abstract
Controlling the timing and local retention of delivered cells remains a major challenge in scaffold-based tissue regeneration, particularly when a mechanically stable scaffold must also permit subsequent cell loading. Here, we present a staged cell delivery strategy that separates scaffold implantation from cell administration by integrating a 3D-printed composite scaffold with an injectable macromolecular carrier phase. Bone marrow mesenchymal stromal cells were delivered to pre-implanted PCL/PEG/chitosan/hydroxyapatite scaffolds using a gelatin/alginate suspension containing cell-laden microcarriers. Chitosan was incorporated to modify the scaffold surface and interfacial properties, while the gelatin/alginate phase provided a shear-thinning injectable matrix for microcarrier delivery. PEG leaching generated a population of surface micropores with a mean width of 23.8 ± 13.5 μm, with 77.0% of the measured pores falling within 10-30 μm. A controlled ex vivo flow-through washout assay showed that PEG-leached scaffolds released substantially fewer microcarriers than non-leached formulations, with the lowest detached counts observed for iP70C5 and iP70C5H5. Together with the composition-dependent adhesion behavior, these findings support contributions from both microscale physical confinement and scaffold-matrix interfacial interactions to microcarrier retention. CCK-8 indicated rBMSC metabolic activity; fluorescence imaging showed L929 viability and spreading in vitro. In a 6-mm rat calvarial defect model, delayed cell delivery on day 7 resulted in a higher bone volume fraction at 12 weeks than delivery on day 1, reaching a BV/TV of 68.0 ± 3.2%. Together, these findings demonstrate that integrating macromolecule-mediated interfacial functionality with scaffold microporosity can support localized retention and staged delivery of cell-laden microcarriers for bone regeneration.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Electrosprayed gelatin-functionalized pectin/sodium alginate microcarriers with controlled degradation for bench-scale 3D suspension culture.Biomaterials advances · 2026
- Engineering a Thiolated Polymeric Nanocomposite Scaffold With Chitosan Nanoparticles for Enhanced OsteogenesisPolymers for Advanced Technologies · 2026
- Core-shell microsphere structure stimulation: Effects on cell behavior and collagen synthesis for regenerative applications.Colloids and surfaces. B, Biointerfaces · 2026
- Load-responsive release of mesenchymal stromal cell extracellular vesicles from polycaprolactone scaffoldsJournal of Biological Engineering · 2026
- Revitalizing bioinert PCL: A biomimetic 3D-Printed gradient-pore scaffold with CSMA hydrogel-mediated BMP-2/QK delivery for vascularized bone regeneration.Journal of biomaterials applications · 2026
- Chitosan molecular weight modulates degradation behavior and osteoblast response in gelatin/PRF hydrogels for craniofacial bone regeneration.Journal of biomaterials applications · 2026