International journal of biological macromolecules

Structure-property insights of ZnO-embedded poly(acrylamide-co-itaconic acid) hybrid networks functionalized with carboxymethyl cellulose, collagen, L-arginine, or dextrin.

Zuhal Akyol, Nermin Orakdogen

Graduate School, Chemistry, Istanbul Technical University, 34469, Istanbul, Turkey. · Faculty of Science and Letters, Department of Chemistry, Soft Materials Research Laboratory, Istanbul Technical University, 34469, Maslak, Istanbul, Turkey. Electronic address: orakdogen@itu.edu.tr.

Key points

From the paper's conclusion
  • Alternating pH between 2.1 and 11.2 produced highly reversible swelling/deswelling transitions associated with protonation/deprotonation of itaconic acid groups.

Abstract

Integration of various organic components systematically modulates the macroscopic properties of zinc oxide@poly(acrylamide-co-itaconic acid)-mace (ZnO@PAIM) anionic gels. The effects of structurally diverse auxiliary components; carboxymethyl cellulose (CMC), collagen (COL), L-arginine (ARG), and dextrin (DEX) were investigated in terms of equilibrium swelling, polymer-solvent interaction parameter χ, and compressive modulus in the as-prepared G₀ and swollen G states. Due to cryoconcentration effect, freeze-polymerized cryogels formed at -18 °C exhibited restricted swelling and 2- to 4-fold mechanical enhancement, reaching 1419.2 ± 162.9 Pa for ARG-integrated hybrid cryogels. Swelling ratios followed Blank > ARG > DEX > CMC > COL, consistent with increasing χ values toward theta threshold (χ ≈ 0.5). COL-integrated hybrids showed lowest swelling and highest χ value (0.4656 ± 0.0012), accompanied by a moderate effective cross-linking density (νe = 6.146 ± 0.917 mol/m3). Reflecting short-chain plasticization, ZnO@PAIM-DEX hybrids exhibited lowest cross-linking efficiency and highest network chain length (N = 22,456.1 ± 4651.7). CMC-integrated hydrogels retained highest as-prepared stiffness despite swelling-induced network relaxation (G < G₀), with a restricted molecular weight between cross-links (Mc = 142.90 ± 23.73 kg/mol). Regarding responsive swelling behavior, increasing NaCl concentration from 10-5 to 1.0 M caused 9.1-, 5.7-, and 4.3-fold volume reductions in Blank, CMC-, and COL-integrated hybrids, respectively. Alternating pH between 2.1 and 11.2 produced highly reversible swelling/deswelling transitions associated with protonation/deprotonation of itaconic acid groups. These dynamic features highlight the reversible stimuli-responsive adaptability of anionic ZnO@PAIM gels, demonstrating their potential for advanced flexible hybrid platforms with tunable elasticity for emerging smart material applications.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers