Electrospun silk sericin-poly(lactic acid) coaxial nanofiber scaffold for esmolol and ferulic acid co-delivery in expedited diabetic wound healing.
Giriraj Pandey, Tejaswini Kolipaka, Deepankar Yadav, Dilip Kumar Arya, Vivek Phatale, Pooja Khairnar, Suraj Wagh, Prashant Pandey,
Pharmaceutical Innovation and Translational Research Lab (PITRL), Department of Pharmaceutics, National Institute of Pharmaceutical Education and Research (NIPER), Hyderabad, 500037, India. · Department of Pharmaceutics, National Institute of Pharmaceutical Education and Research (NIPER), Kolkata, 700054, India.
Key points
From the paper's conclusion- Therefore, we have developed a ferulic acid (FA)-esmolol (ESM)-loaded coaxial nanofibrous (NFs) scaffold using silk sericin (SS) as the shell and poly(lactic acid) (PLA) as the core via electrospinning for DFU management.
Abstract
Diabetic foot ulcers (DFUs) are chronic, infection-prone wounds that heal poorly due to impaired angiogenesis, persistent inflammation, and elevated oxidative stress, creating a substantial clinical and economic burden and highlighting the need for advanced extracellular matrix-mimicking dressings. Therefore, we have developed a ferulic acid (FA)-esmolol (ESM)-loaded coaxial nanofibrous (NFs) scaffold using silk sericin (SS) as the shell and poly(lactic acid) (PLA) as the core via electrospinning for DFU management. The optimized scaffold showed a uniform, bead-free morphology with increased fiber diameter (370 ± 95 nm) compared to blank NFs (201 ± 52 nm) and a confirmed core-shell architecture. The FA-ESM NFs demonstrated high porosity (81.04 ± 4.39%) and an optimal water vapor transmission rate (WVTR) (2077 g/m2/day), supporting a moist wound environment. Water retention (409.39 ± 12.41%) and controlled biodegradation (~98% over 21 days) indicated excellent exudate handling and sustained structural integrity. Mechanical analysis showed suitable tensile strength (1.20 MPa) and elongation (112.80%). Drug release followed the Korsmeyer-Peppas model (R2 ≈ 0.975/0.9811; n = 0.699/0.883), indicating anomalous to case II transport. The scaffold exhibited significant antioxidant activity, >80% cell viability, and hemocompatibility. It significantly enhanced cell migration within 48 h and modulated biomarkers (↓MMP-9, ↓TNF-α, ↑VEGF; p < 0.01). Strong antibacterial activity against Staphylococcus aureus and Pseudomonas aeruginosa, along with significantly accelerated wound closure in diabetic models within 16 days (p < 0.0001), further validates its therapeutic efficacy. Overall, the scaffold demonstrates promising anti-inflammatory, antioxidant, and pro-angiogenic properties and potentially effective dressing for DFU management.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fabrication and Healing Potential of Polylactic Acid /Clay/Nd2O3 Nanocomposite Fibers in Diabetic Wound Therapy.Macromolecular bioscience · 2026
- Sustained in situ exosome delivery reprograms the diabetic wound microenvironment to unlock immuno-angiogenic repair.Regenerative biomaterials · 2026
- Sustainable Electrospun PCL Nanofibers Reinforced With Eggshell Membrane for Prolonged Cu (II) Complex Release and BioactivityMacromolecular Materials and Engineering · 2026
- Phytoextract-loaded bioinspired PLGA nanofibrous scaffold promotes diabetic wound healing via anti-inflammatory and antioxidant effects in in vitro and in vivo experimental models.Journal of molecular histology · 2026
- Antibacterial and immunomodulatory core-shell nanofibrous membranes accelerate skin wound repair and regeneration.Burns : journal of the International Society for Burn Injuries · 2026
- Quantitative Mechanophysical Correlations Governing Antibacterial Performance of Amoxicillin-Loaded Poly(ε-caprolactone)/Poly(ethylene glycol) Biodegradable Electrospun Nanofibrous Wound DressingPolymers · 2026