Environmental research

Thermal activation and antisolvent regulation enable integrated LiCoO2 leaching and selective cobalt separation in a high-viscosity deep eutectic solvent.

Guangke Ye, Yunxia Wu, Guofan Zhang

School of Minerals Processing and Bioengineering, Central South University, Changsha 410083, China. · School of Minerals Processing and Bioengineering, Central South University, Changsha 410083, China. Electronic address: 245601030@csu.edu.cn.

Key points

From the paper's conclusion
  • These results establish a solvent-process co-design strategy in which temperature addresses transport limitations while antisolvent regulation controls downstream metal partitioning, thereby broadening DES design beyond viscosity minimization.

Abstract

Recovering critical metals from spent lithium-ion batteries requires solvent systems that couple rapid cathode dissolution with selective downstream separation. Most deep eutectic solvent (DES) recycling strategies prioritize viscosity reduction, although compositional changes made to achieve lower viscosity can also alter the chemical functions governing dissolution and metal speciation. Here, a hydrated cetylpyridinium chloride monohydrate-lactic acid DES (CL-DES; 1:4 mass ratio; 440 mPa·s at 25 °C) was coupled with thermal activation and ethanol-induced antisolvent precipitation for LiCoO2 recycling. At 150 °C, CL-DES leached 99.72% of Li and 99.25% of Co within 30 min, exceeding the nominal-LA-loading-matched LA-H2O control by 23.90 and 35.41 percentage points, respectively. Avrami-Erofeev analysis of the kinetically active portion of the Co-leaching curves yielded temperature-dependent rate constants and an apparent activation energy of 83.3 kJ∙mol-1. FTIR, XPS, EPR, UV-vis spectroscopy, and microscopy collectively supported proton-assisted lattice destabilization, Co(III)-to-Co(II) reduction, and stabilization of dissolved cobalt in chloride- and carboxylate-containing coordination environments. After ethanol was added at 1.5 times the leachate mass, the absorption bands associated with chloride-coordinated Co(II) species disappeared from the filtrate; 99.81% of Li remained in the filtrate, whereas the fraction of Co remaining in the filtrate decreased to 1.98%, corresponding to an apparent liquid-phase Co removal of 98.02%. The recovered precipitate was subsequently converted to an XRD-identified Co3O4 product. CL-DES additionally achieved 99.4-99.7% leaching of Li, Co, Ni, and Mn from NMC532 at 150 °C. These results establish a solvent-process co-design strategy in which temperature addresses transport limitations while antisolvent regulation controls downstream metal partitioning, thereby broadening DES design beyond viscosity minimization.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers