Insights into the mechanism and chloride immobilization of seawater-mixed alkali-activated materials.
Yunhong Tang, Kim Hung Mo, Henglong Zhang, Lei Wang, Zhenyu Tan, Yao Luo
Department of Civil Engineering, Faculty of Engineering, Universiti Malaya, 50603 Kuala Lumpur, Malaysia. · Research Centre for Carbon Dioxide Capture and Utilisation (CCDCU), Faculty of Engineering and Technology, Sunway University, No. 5, Jalan Universiti, Bandar Sunway 47500, Selangor Darul Ehsan, Malaysia. Electronic address: khmo@sunway.edu.my.
Key points
From the paper's conclusion- Chloride immobilization occurs through both chemical binding and physical adsorption.
Abstract
Freshwater scarcity and the carbon intensity of cement production represent two major environmental challenges. Seawater-mixed alkali-activated materials (AAMs), incorporating industrial and agricultural by-products, offer opportunities to reduce reliance on freshwater and cement. However, seawater cannot be regarded as an inert substitute for freshwater because its multi-ionic composition fundamentally alters alkali activation. This review examines the competing mechanisms arising from interactions among seawater, precursors, and alkali activators, with emphasis on differences in reaction kinetics, phase evolution, and chloride immobilization between high- and low-calcium AAMs. Competing mechanisms are primarily governed by precursor, ion concentrations, and activator chemistry. In high-calcium AAMs, chloride can promote calcium dissolution and accelerate early reactions, but its accelerating effect is concentration-dependent and might be counteracted by Mg-induced alkalinity reduction and premature precipitation. In contrast, low-calcium AAMs lack a Ca-driven acceleration mechanism and rely mainly on aluminosilicate dissolution, which might make them potentially more susceptible to Mg-induced alkalinity reduction. In addition, High-calcium AAMs favor C-A-S-H gels and chloride-bearing phases such as Friedel's salt and layered double hydroxides, whereas low-calcium AAMs are dominated by N-A-S-H gels, with potential zeolitic transformations. Chloride immobilization occurs through both chemical binding and physical adsorption. Notably, higher calcium content does not necessarily ensure superior chloride-binding capacity, highlighting the importance of reactive amorphous phase ratios rather than precursor type alone. Understanding these coupled mechanisms is essential for designing seawater-compatible AAMs that support freshwater-saving and low-carbon construction.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Unveiling hydration pathways and kinetics of red mud-derived cementitious materials via tailored alkali activation systems.Waste management (New York, N.Y.) · 2026
- Influence of Seawater-Derived Salts on Ye’elimite Hydration Kinetics and Microstructural Evolution: Toward Developing Sustainable Calcium Sulfoaluminate Cement-Based MaterialsACS Sustainable Chemistry & Engineering · 2026
- Interaction of plant particles / fibres and alkali activated materials: Critical review, unsolved problems and future direction of research.Environmental research · 2026
- Mechanical and microstructural properties of pre-treated incinerator bottom ash as fly ash replacement in alkali-activated materialsMaterials and Structures · 2026
- Regulating Silicate Speciation and Geopolymerization Kinetics through Crystalline Water in Solid Sodium Silicate Activator.ACS omega · 2026
- Evolution of Hydration Gel Phases and Microstructure in Alkali-Activated Binders with Varied Calcium Contents.Materials (Basel, Switzerland) · 2026