Reconciling competing objectives in carbonated MSWI fly ash washing: Dechlorination, calcium retention, and heavy metal stabilization.
Xuyang He, Jincheng Wang, Dingyuan Zhang, Weihua Li, Xue Li, Yingjie Sun, Ying Zhu, Rongxing Bian,
Qingdao Solid Waste Pollution Control and Resource Engineering Research Center, Qingdao University of Technology, School of Environmental and Municipal Engineering, Qingdao, 266033, China; The State Key Laboratory of Pollution Control and Resource Reuse, School of Environmental Science and Engineering, Tongji University, Shanghai, 200092, China. · Qingdao Solid Waste Pollution Control and Resource Engineering Research Center, Qingdao University of Technology, School of Environmental and Municipal Engineering, Qingdao, 266033, China.
Key points
From the paper's conclusion- Overall, the coupled treatment alleviated the trade-offs among chloride removal, calcium retention, and heavy metal stabilization, thereby improving the resource recovery potential of treated fly ash.
Abstract
The resource utilization of MSW incineration fly ash is constrained by its high chloride content, calcium loss during washing, and the environmental risk of residual heavy metals. This study proposes a multistage pretreatment integrating carbonation, ball milling, ultrasonication, and CO2-coupled washing to balance dechlorination, calcium retention, and heavy metal stabilization. Citric acid (CA), ammonium bisulfate (AB), and ethylenediaminetetraacetic acid (EDTA) were selected as washing agents and evaluated on carbonated fly ash. For the investigated fly ash, results demonstrated that carbonation provided the foundational calcium fixation, while ball milling physically disrupted particle agglomerates to expose encapsulated chlorides, with 60 min selected as the milling duration. Ultrasonication for 10 min further reduced soluble chloride contents in heavily carbonated fly ash residues to 0.72%, 0.79%, and 0.81%, respectively, with calcium loss rates of 14.30%, 10.81%, and 12.08%. However, EDTA washing caused severe remobilization of Pb, Zn, Cu, and Cd. Further coupling ball milling and ultrasonication with in-situ CO2 sparging (20 min for CA and 10 min for AB) improved the overall treatment performance. The lowest soluble chloride content (0.71%) was obtained with CA, whereas AB achieved the lowest calcium loss (8.87%). All heavy metal leaching concentrations in CA and AB residues met the regulatory limits. Risk assessment code analysis indicated that AB generally resulted in lower environmental risks than CA, although Cd remained the primary residual concern. Overall, the coupled treatment alleviated the trade-offs among chloride removal, calcium retention, and heavy metal stabilization, thereby improving the resource recovery potential of treated fly ash.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- In situ mechanochemical carbonation enables carbon-negative detoxification and upcycling of municipal solid waste incineration fly ash.Environmental research · 2026
- Synergistic stabilization of heavy metals in MSWI fly ash using Ca-bearing chitosan and CFBC fly ash.Environmental science and pollution research international · 2026
- Water-washing pretreatment enhanced co-smelting of MSWI fly ash and copper slag: Metals extraction, slag vitrification and silicate network evolution mechanism.Journal of hazardous materials · 2026
- Hydration and Molecular Dynamics Simulation of Carbonated and Hydrophobically Modified Municipal Solid Waste Incineration Fly Ash Mortars.Materials (Basel, Switzerland) · 2026
- Advancements in Detoxification of Municipal Solid Waste Incineration Fly Ash: A Review of Hazardous Properties, Treatment Strategies, and Resource UtilizationMaterials · 2026
- Bioleaching of heavy metals from municipal solid waste incineration fly ash by Penicillium citrinum and analysis of associated metabolites.Journal of hazardous materials · 2026