Hemihydrate phosphogypsum as a waste-derived sulfate source for low-carbon supersulfated cement: Hydration regulation and strength-normalized environmental performance.
Zhengning Sun, Boxin Wang, Yibing Zuo, Ru Mu, Heng Chen, Jiahuan Guo
State Key Laboratory of Deep Earth Exploration and Imaging, College of Construction Engineering, Jilin University, Changchun, 130026, China. Electronic address: sunzn23@mails.jlu.edu.cn. · State Key Laboratory of Deep Earth Exploration and Imaging, College of Construction Engineering, Jilin University, Changchun, 130026, China. Electronic address: boxinwang@jlu.edu.cn.
Key points
From the paper's conclusion- Hemihydrate phosphogypsum (HPG) can serve as a waste-derived sulfate source in low-clinker supersulfated cement (SSC), expanding phosphogypsum utilization while reducing demand for natural gypsum.
Abstract
Hemihydrate phosphogypsum (HPG) can serve as a waste-derived sulfate source in low-clinker supersulfated cement (SSC), expanding phosphogypsum utilization while reducing demand for natural gypsum. This study examines how HPG content governs the temporal evolution of sulfate supply and how this evolution relates to hydration, pore structure, and long-term strength in SSC co-activated with ferroaluminate clinker (FAC), carbide slag (CS), and sodium silicate (SS). Mixtures containing 5-25 wt% HPG were evaluated for compressive strength. The 10, 15, and 20 wt% HPG mixtures were further analyzed by hydration kinetics, pore-solution chemistry, quantitative phase analysis, and microstructural characterization. Composite-activated SSC developed 10.23-14.36 MPa at 1 d, corresponding to a 205.4-328.7% increase over the CS-activated reference. The 15 and 20 wt% HPG mixtures reached 65.54 and 63.76 MPa at 28 d and continued to increase to 81.56 and 78.79 MPa at 270 d, respectively. At 10 wt% HPG, sulfate depletion after early hydration constrained continued ettringite formation and late-age pore refinement. At 20 wt% HPG, sustained reaction of ground granulated blast-furnace slag (GGBS) generated slightly more ettringite and C-(A)-S-H, but a larger fraction of pores >50 nm remained, diminishing the strength efficiency of the additional hydration products. The 15 wt% HPG mixture provided the most favorable coupling of sulfate supply, hydrate accumulation, pore refinement, and strength, and achieved the lowest 28 d energy- and carbon-intensity indices among the investigated mixtures.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Synergistic mechanism of desulfurization gypsum and carbide slag in no-clinker supersulfated cementCase Studies in Construction Materials · 2026
- Superplasticizer Incompatibility in SuperSulfated Cement Containing BYF Clinker: Hydration, Microstructure, and Strength Developmentce/papers · 2026
- Mineral reconstruction of high-volume phosphogypsum driven by a slag-based composite stabilizer: mechanisms of subgrade performance enhancement and phosphorus/fluoride immobilization.Journal of hazardous materials · 2026
- Mechanistic Understanding of Early Strength Development and Shrinkage Mitigation in Low-Clinker High-Volume Slag Binders: Further Performance Enhancement Through Particle Packing Optimization Under Desulfurization Gypsum ActivationMaterials · 2026
- Coupling limestone powder with CFSH/PCE to enhance supersulfated cement: Hydration, microstructure and carbonation resistance.Environmental research · 2026
- The Directional Regulation and Performance Enhancement Mechanism of Composite-Activated Biomass Power Plant Ash on All-Solid-Waste Eco-Friendly Supersulfated Cement.Environmental research · 2026