NaCl-induced crystallization for Na2SiF6 recovery from real glass-thinning etching wastewater.
Zipeng Zhang, Kangping Cui, Libei Zhu, Jiao Wang, Youde Zhang
School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China. · School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China. Electronic address: cuikangping@hfut.edu.cn.
Key points
From the paper's conclusion- This study developed a NaCl-induced crystallization-recrystallization process for selective Na2SiF6 recovery and evaluated NaCl dosage, stirring time, temperature, and recrystallization solid-to-liquid ratio.
Abstract
Recovering resources from real glass-thinning etching wastewater is challenging because of its high acidity and complex ionic composition. This study developed a NaCl-induced crystallization-recrystallization process for selective Na2SiF6 recovery and evaluated NaCl dosage, stirring time, temperature, and recrystallization solid-to-liquid ratio. The wastewater contained 29.439 g L-1 total F, 3.269 g L-1 dissolved Si, and 4.33 mol L-1 total acidity. At an NaCl dose of 1.2 times the stoichiometric requirement, 40 °C, and 45 min, primary crystallization achieved a dissolved-Si-based H2SiF6-equivalent removal efficiency of 95.50 ± 0.08% and crude-product purity of 91.30 ± 1.26%. The Avrami model empirically described the depletion kinetics (R2 = 0.99991). Recrystallization at 1:75 (g:mL) provided approximately 55% stage dry-mass recovery and increased Na2SiF6 purity to 99.52 ± 0.08 wt%, meeting GB/T 23936-2018 requirements. An apparent F-Si mass balance showed that the final product retained 24.54 ± 0.19% of wastewater-input F and 51.19 ± 1.91% of wastewater-input Si, distinguishing elemental recovery from liquid-phase removal and product purity. XRD, FTIR, and Raman identified Na2SiF6 as the predominant phase. Thermal decomposition occurred mainly at 500-620 °C and yielded NaF as the predominant detectable solid product. Because the primary mother liquor retained high total-F, SO42-, Cl-, and acidity loads, the process should be regarded as a front-end resource-recovery step requiring downstream mother-liquor treatment.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Electrocoagulation-crystallization synergistic regulation for efficient fluoride removal and cryolite recovery from simulated photovoltaic wastewater.Environmental technology · 2026
- Stepwise pH-Regulated Homogeneous Crystallization Enables Selective Phosphorus Recovery from Hydrothermally-Leached Sludge toward Value-Added Material SynthesisACS ES&T Water · 2026
- From waste to functional products: Controlled recovery of calcium fluoride and lithium sulfate monohydrate from phosphogypsumNext Materials · 2026
- Phosphorus recovery from high-COD and strongly acidic wastewater by vivianite crystallization: feasibility and optimization of operating conditionsFrontiers in Chemistry · 2026
- Efficient Phosphate Recovery via Membrane-Free Electrochemical Separation Coupled with Fluidized Bed Crystallization: A Long-Term Operation and Comprehensive Demembranization SolutionEnvironmental Science & Technology · 2026
- Electrochemical Activation of Natural Magnesite for Phosphorus Recovery from Wastewater via In Situ Struvite Crystallization.Molecules (Basel, Switzerland) · 2026