Non-isothermal sintering of dental zirconia for enhanced flexural strength and workflow efficiency without compromising translucency.
Leticia V S Souza, Rena R Liu, Amin Shaker, Abdulaziz M Alshahrani, Mirelle M Ruggiero, Zheng Li, Vanessa Cavalli, Yu Zhang
Laboratories for Microstructure Physics & Mechanics of Materials, Department of Preventive and Restorative Sciences, School of Dental Medicine, University of Pennsylvania, Philadelphia, PA, USA; Department of Restorative Dentistry, University of Campinas - Piracicaba Dental School, Piracicaba, SP, Brazil. · Laboratories for Microstructure Physics & Mechanics of Materials, Department of Preventive and Restorative Sciences, School of Dental Medicine, University of Pennsylvania, Philadelphia, PA, USA; Department of Biological Sciences, Lehigh University, Bethlehem, PA, USA.
Key points
From the paper's conclusion- n-IS using higher sintering temperatures, low and constant heating and cooling rates, and no dwell time is recommended to increase the strength of 3YSZ, 4YSZ, and 5YSZ while maintaining good optical properties and reducing laboratory processing time.
Abstract
OBJECTIVES: To determine whether long dwell times in conventional isothermal sintering (CIS) are necessary to achieve desirable properties in yttria-stabilized zirconia (YSZ) for dental restorations using a non-isothermal sintering (n-IS) protocol, i.e., without dwell time at the sintering temperature. METHODS: 300 disc-shaped specimens (n = 10) were cold-isostatically pressed from 3YSZ (Zpex), 4YSZ (Zpex 4), and 5YSZ (Zpex Smile) powders (Tosoh Corp.) and sintered at 1350, 1400, 1450, 1500, and 1550 °C using either CIS (2-h dwell) or n-IS (0-min dwell), with constant heating and cooling rates of 5 °C/min. Density, phase content, microstructure, translucency parameter, and biaxial flexural strength were evaluated. Data, except for grain size and phase analyses (n = 1 for each), were analyzed using one-way ANOVA followed by Tukey's test (α = 0.05). RESULTS: n-IS at high sintering temperatures produced densification comparable to that of CIS (>99%) for all three YSZ compositions (p > 0.05). n-IS yielded higher tetragonal phase content and smaller grain sizes in all three YSZ compositions relative to CIS. The translucency of 3YSZ was not affected by the sintering protocol at higher temperatures (p > 0.05); however, 4YSZ and 5YSZ exhibited lower translucency with n-IS (p < 0.05). n-IS significantly improved the flexural strength of all YSZ compositions compared with CIS (p < 0.05). CONCLUSIONS: n-IS using higher sintering temperatures, low and constant heating and cooling rates, and no dwell time is recommended to increase the strength of 3YSZ, 4YSZ, and 5YSZ while maintaining good optical properties and reducing laboratory processing time.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of sintering programs on microstructure, crystal phase composition, and optical and mechanical properties of multilayer zirconia.Dental materials : official publication of the Academy of Dental Materials · 2026
- Effects of high-speed sintering on the translucency and color of dental zirconia with different shades and yttria contents.Journal of prosthodontics : official journal of the American College of Prosthodontists · 2026
- Influence of speed sintering on the mechanical properties of layer-free multi-layer zirconia.Dental materials journal · 2026
- Influence of non-thermal atmospheric plasma on the mechanical properties and phase stability of zirconia ceramics.Dental materials : official publication of the Academy of Dental Materials · 2026
- Cold‐Sintering Pretreatment for Energy‐Efficient Densification of 3YSZ via Macropore‐to‐Mesopore TransformationInternational Journal of Applied Ceramic Technology · 2026
- Optical properties of conventional and high-translucency zirconia ceramics and their effects on resin cement polymerization.Journal of dental sciences · 2026