Biomaterials

Rare-earth-free magnesium-zinc alloy with controlled biodegradation and biocompatibility for novel biodegradable metallic stent.

Yubeen Park, Yerin Ha, Hyung Jin Roh, Hyun Lee, Seung Jin Eo, Do-Yoon Kang, Nayoung Lee, Hyun-Do Jung,

Biomedical Engineering Research Center, Asan Institute for Life Sciences, Asan Medical Center, 88 Olympic-ro 43-gil, Songpa-gu, Seoul, 05505, Republic of Korea. · Biomedical Engineering Research Center, Asan Institute for Life Sciences, Asan Medical Center, 88 Olympic-ro 43-gil, Songpa-gu, Seoul, 05505, Republic of Korea; Department of Medical Science Convergence, Graduate School of Medical Science, University of Ulsan, 93, Daehak-ro, Nam-gu, Ulsan, 44610, Republic of Korea; Department of Convergence Medicine, Asan Medical Center, University of Ulsan College of Medicine, 88 Olympic-ro 43-gil, Songpa-gu, Seoul, 05505, Republic of Korea.

Key points

From the paper's conclusion
  • Collectively, these findings define a composition-microstructure-corrosion-cellular response-vascular healing axis and identify MZ01 as a RE-free Mg-Zn alloy with controlled biodegradation and favorable biocompatibility, supporting its further development as a biodegradable cardiovascular scaffold.

Abstract

Biodegradable magnesium (Mg) alloy stents offer a transient alternative to permanent metallic implants; however, clinically used WE43 contains rare-earth (RE) elements, raising concerns regarding the long-term biosafety of RE-containing degradation products and their potential tissue accumulation. Here, we investigated two RE-free Mg-Zinc (Zn)-based alloys, MZ01 (Mg-1Zn-0.1Ca) and ZM115 (Mg-1Zn-1.5Mn-0.5Sr), and established a mechanistic cascade linking alloy composition and microstructure to electrochemical analyses revealed alloy-dependent differences in grain structure and interfacial corrosion resistance, with MZ01 exhibiting the highest charge-transfer resistance. In a mouse subcutaneous model, MZ01 showed more uniform degradation, smaller and more rapidly resolving hydrogen gas cavities, and a significantly lower microcrack area fraction at Day 56 than WE43 and ZM115, accompanied by attenuated inflammatory and fibrotic responses. In the rabbit iliac arteries, all stents maintained luminal patency without thrombosis through 56 days, while MZ01 exhibited lower neointimal thickness, lower perivascular apoptosis and late inflammation, and enhanced early endothelialization compared with WE43. Preliminary descriptive porcine coronary implantation further demonstrated the technical feasibility and sustained patency of MZ01 over 56 days. Collectively, these findings define a composition-microstructure-corrosion-cellular response-vascular healing axis and identify MZ01 as a RE-free Mg-Zn alloy with controlled biodegradation and favorable biocompatibility, supporting its further development as a biodegradable cardiovascular scaffold.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers