A comparative review of concrete properties using waste materials as natural coarse aggregate substitutes
Md Faiyaz Shahriar, Takia Kamal
Key points
From the paper's conclusion- Substituting coarse aggregate alone alters cradle-to-gate CO₂ by approximately − 6% to + 6%, and for recycled coarse aggregate a small increase of 0.3–3.4% has been reported.
Abstract
Natural aggregate is being extracted faster than it is replaced, while mineral and industrial waste continues to accumulate. This review synthesizes the published evidence on fourteen waste materials used as partial or full replacements for natural coarse aggregate in concrete: recycled concrete, crushed brick, ceramic, waste glass, plastic, tyre rubber, sintered fly-ash lightweight aggregate, coconut shell, oil-palm shell, steel slag, waste marble, granite waste, coal bottom ash and e-waste. Of 538 records identified, 154 studies met the eligibility criteria. Only investigations that replaced coarse aggregate and reported a natural-aggregate control contributed to the comparative synthesis; fine-aggregate and binder-replacement studies were retained solely to explain mechanisms. A three-family classification is proposed on the basis of density, porosity and surface chemistry: dense and low-porosity streams (steel slag, marble, granite, glass, vitrified ceramic), porous and water-absorbing streams (recycled concrete, brick, sintered fly-ash aggregate, bottom ash, bio-based shells), and polymeric and hydrophobic streams (plastic, rubber, e-waste). Dense, low-porosity streams maintained or increased strength and reduced the transport of water and ions. Porous streams reduced hardened density by approximately 25–30% and increased absorption, with most investigations limiting replacement to 20–30% for structural applications. Polymeric streams reduced strength substantially while increasing ductility and, for rubber, frost resistance. Three qualifications apply: steel slag is chemically reactive and potentially expansive, marble is soluble in acid, and e-waste is compositionally variable. Durability evidence remains sparse and heterogeneous in exposure conditions, so it is reported as descriptive evidence with the number of contributing studies stated. Substituting coarse aggregate alone alters cradle-to-gate CO₂ by approximately − 6% to + 6%, and for recycled coarse aggregate a small increase of 0.3–3.4% has been reported. Reductions of approximately 17% derive from partial clinker substitution rather than from aggregate replacement.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Utilization of Locally Available Waste Material for Sustainable ConstructionRecent Research Reviews Journal · 2026
- Valorization of Quarry Sludge Waste as a Complete Fine‐to‐Coarse Lightweight Aggregate System for Structural ConcreteJournal of the American Ceramic Society · 2026
- The impact of combined recycled coarse aggregates from non-hazardous construction and demolition waste on self-compacting concrete performance for sustainable constructionCleaner Waste Systems · 2026
- Mechanical and Environmental Performance of Circular Concrete with Recycled Aggregates from Composite Material Waste.ACS omega · 2026
- Developing High-strength, Flowable Sand Concrete by Adding Combined Industrial Ceramic and Granite Waste with Seashell Bio-waste as Fine AggregatesPeriodica Polytechnica Chemical Engineering · 2026
- Hardened Properties of Eco-Friendly Concrete Using Crushed Waste Shells as All Fine Aggregates.Materials (Basel, Switzerland) · 2026