Binary effect of silica fume and waste glass powder as a cement replacement for a sustainable concrete
Ömer Damdelen, Mohammad Ali Mosaberpanah, Stephen Babajide Olabimtan, Micheal Deric Anthony, Babatunde Olufunso Oluwole
Cyprus International University
Key points
From the paper's conclusion- This study demonstrates that incorporating GP and SF enhances concrete performance, reduces environmental impact, and offers a sustainable and practical solution for modern construction applications.
Abstract
One promising implementation entails the utilization of silica fume and waste glass powder. This study aims to examine the impact of incorporating twelve different combinations of Glass Powder (GP) and Silica Fume (SF) as partial cement replacements in concrete mixtures. The experimental proportions include individual replacements of GP (5%, 10%, 15%, 20%) and SF (5%, 10%, 15%, 20%), along with blended combinations (GP 20%-SF 20%, GP 10%-SF 10%, GP 20%-SF 10%, GP 10%-SF 20%, GP 15%-SF 15%, GP 15%-SF 5%, and GP 5%-SF 15%). A thorough experimental investigation was conducted to examine key concrete properties, encompassing fresh state (workability), hardened state performance (compressive and tensile strength), durability indicators (water absorption and density), microstructural features (SEM), and elevated temperature resistance. Among the tested mixes, mix 10 (20% GP & 20% SF) demonstrated the highest slump compared to the control mix. Meanwhile, mix 5 (15% SF) achieved the greatest compressive strength, showing a 9.5% improvement over the control mix. This enhancement is due to the pozzolanic reaction of silica fume and glass powder, which refined the microstructure, thereby increasing strength. In terms of splitting tensile strength, mix 5 (15% SF) again performed the best, with a 13.3% increase over the control mix. On the other hand, mix 4 (15% GP) had the highest density, exhibiting a 2.6% rise compared to the control. Additionally, mix 3 (10% SF) displayed the lowest water absorption, attributed to the filler effect and pozzolanic activity, which sealed voids and densified the matrix, reducing water penetration into the samples. At 400 °C, mix M10 exhibited the highest residual compressive strength of 46.32 MPa, relative to the 28-day strength of the unexposed control, whereas mix M5 showed the lowest value of 38.34 MPa. This study demonstrates that incorporating GP and SF enhances concrete performance, reduces environmental impact, and offers a sustainable and practical solution for modern construction applications.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Sustainable Concrete Production Using Fly Ash and Recycled Glass Powder: Environmental and Mechanical Performance EvaluationSustainability · 2026
- Effect of Waste Glass Powder as a Cementitious Material in ConcreteIOP Conference Series: Earth and Environmental Science · 2026
- Development of Sustainable Concrete Using Marble Waste Powder and Silica FumeIOP Conference Series: Earth and Environmental Science · 2026
- Glass as a sustainable supplementary material in cementitious and geopolymer composites: a reviewJournal of Sustainable Cement-Based Materials · 2026
- Mechanical performance and eco-strength efficiency of sustainable concrete incorporating supplementary cementitious materials (SCMs), glass powder, and recycled plasticDiscover Concrete and Cement · 2026
- Synergic utilization of waste glass powder for fire-resilient and low alkali-activated concreteScientific Reports · 2026