Statistical modeling and multi response optimization of wire electrical discharge machining of Haynes 230 with validation through microstructural characterization
Gurnam Singh, Neel Kanth Grover, Vivek Aggarwal
Key points
From the paper's conclusion- Composite microhardness increased from a bulk matrix baseline of 427–534 HV within high-energy zones, driven by ultra-rapid solidification rates, micro-segregation of secondary phases, and severe quench-induced strengthening.
Abstract
Haynes 230, a high-temperature Ni–Cr–W–Mo superalloy valued for its oxidation resistance and thermal stability, exhibits severe deformation-induced hardening and tool wear during conventional machining. However, the machinability of this specific alloy under wire electrical discharge machining regimes remains largely uninvestigated. This study establishes a comprehensive response surface framework to systematically evaluate the independent and interactive influences of pulse-on time (On-Tp), pulse-off time (Off-Tp), peak current (Ip), spark-gap voltage (GVs), wire feed rate (FRw), and wire tension (Tw) on cutting rate (CR) and surface roughness (SR). ANOVA identified GVs and On-Tp as the primary governing factors dictating plasma channel dynamics. Multi-response desirability optimization successfully established an equilibrium processing window, yielding a validated, stable performance of CR = 1.80 mm/min and SR = 1.66 μm. Subsurface integrity is highly sensitive to variations in discharge energy density. The recast layer thickness altered from 10.6 μm under CR-optimized conditions to 2.4 μm under SR-optimized conditions, and was restricted to 4.85 μm within the multi-response optimized window. Characterization of the machined surface confirmed significant element partitioning within this zone, featuring the depletion of matrix constituents (Ni, Cr, Co), the relative enrichment of heavy refractory elements (W, Mo), and the interstitial infusion of oxygen and zinc due to dielectric decomposition and tool-electrode transfer. Composite microhardness increased from a bulk matrix baseline of 427–534 HV within high-energy zones, driven by ultra-rapid solidification rates, micro-segregation of secondary phases, and severe quench-induced strengthening. Ultimately, this work correlates validated macroscopic input boundaries with process-induced metallurgical evolution to establish an optimized, high-integrity manufacturing framework for critical aerospace components.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Performance optimization of wire EDM of Nitinol shape memory alloy using BBD RSM and TLBO with alumina nano graphene and MWCNT Powder mixed dielectricScientific Reports · 2026
- An explainable hybrid RSM–SHAP framework for multi-parameter optimization of WEDM performance in D2 tool steelJournal of Materials Science: Materials in Engineering · 2026
- Microstructural Analysis of Recast Layer Thickness and Microcrack Formation During EDM of Hastelloy C-22 with Different Graphite ElectrodesMaterials · 2025
- ANALYSIS AND OPTIMIZATION OF SURFACE INTEGRITY IN WIRE ELECTRICAL DISCHARGE MACHINING PROCESKufa Journal of Engineering · 2026
- Surface integrity and multi-objective optimization of Ti-6Al-4V alloy by EDM using a WC/Cu powder metallurgy electrode: an integrated RSM–ANN approachMetallurgical Research & Technology · 2026