Distinct Roles of Nanoparticle Incorporation and Polymer Degradation in Fibroblast Response to Device Design.
Kendell M Pawelec, Erik M Shapiro
Department of Radiology, Michigan State University, East Lansing, MI 48824, USA.
Key points
From the paper's conclusion- Together this highlights that scaffold design affects biological response immediately post-implantation in ways that impact the ultimate success or failure of biomedical devices.
Abstract
Fibrotic encapsulation of implanted biomedical devices represents the highest cause of device failure across numerous fields, including orthopedics, breast implants and neural electrodes. While most research has focused on the immune system for driving the foreign body response and ultimate device success, fibroblasts are emerging as another key regulator of tissue response. Therefore, in the present study, we evaluated the activation of primary human dermal fibroblasts into myofibroblasts, a contractile cell that is a hallmark of fibrosis, in response to the design of porous scaffolds mimicking regenerative medicine implants. Over four weeks in culture, two factors were studied (1) nanoparticle incorporation into scaffolds for imaging functionality and (2) the scaffold's polymer matrix, which dictates chemistry, mechanics and degradation. Incorporation of tantalum oxide (TaOx) nanoparticles, a radiopaque nanoparticle able to impart CT-visibility to radiolucent polymers, had a minimal effect on fibroblasts at ≤ 20 wt%, but significantly down-regulated expression of alpha smooth muscle actin (αSMA) (0.31 ± 0.1 fold change) compared to scaffolds without nanoparticles, likely driven by the increase in nanoscale surface roughness. Degradation rate of the polymer matrix altered myofibroblast activation, with a fast-degrading polymer, poly(lactide co-glycolide) (PLGA) 50:50, significantly up-regulating multiple myofibroblast markers, including αSMA (5.16 ± 2.5), vinculin, integrin β 1, and integrin β 5, compared to non-degrading polycaprolactone (PCL). The effect was due to the release of degradation products, namely lactic acid, which affects cellular metabolism. Together this highlights that scaffold design affects biological response immediately post-implantation in ways that impact the ultimate success or failure of biomedical devices.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- In vivo study of the effect of composition and implantation site on scaffold degradation rate.Communications materials · 2026
- Biofabrication and Characterization of Fluorapatite-Coated Poly(lactic-co-glycolic acid) Microscaffolds: Physicochemical Properties and Human Dental Pulp Stem Cell Responses.Journal of functional biomaterials · 2026
- Fabrication and Characterization of a Trans-Activator of Transcription Peptide-Functionalized Collagen-Mineral Trioxide Aggregate Nanofiber Scaffold: Physicochemical Properties and Fibroblast Response.Clinical and experimental dental research · 2026
- TiO₂ Nanoparticles—Incorporated PCL /Gelatin Nanocomposite Fibers for Enhanced Biocompatibility and Reduced Foreign Body ResponseBiopolymers · 2025
- A dual-scale micro/nanofibrous PLGA scaffold fabricated by co-electrospinning for regenerative endodontic procedures.Journal of applied oral science : revista FOB · 2026
- Biomaterial-Activated Macrophage-T Cell Crosstalk Promotes Myofibroblastic Differentiation of Mesenchymal Stem Cells.Journal of biomedical materials research. Part A · 2026