Thermally Exfoliated Graphitic Carbon Nitride-modified Alkaline Electrolyte for Suppressing Parasitic Reactions in Rechargeable Zinc-air Batteries
Mustapha Balarabe Idris, Bhekie B. Mamba, Xolile Fuku
Key points
From the paper's conclusion- Herein, thermally exfoliated graphitic carbon nitride (GCN ex ) is investigated as an electrolyte modifier for mitigating parasitic reactions in concentrated alkaline media.
Abstract
The instability of the zinc/electrolyte interface, arising predominantly from parasitic hydrogen evolution reaction (HER) and zinc corrosion, remains a major limitation to the durability of rechargeable zinc-air batteries (ZABs). Herein, thermally exfoliated graphitic carbon nitride (GCN ex ) is investigated as an electrolyte modifier for mitigating parasitic reactions in concentrated alkaline media. GCN ex is prepared from melamine through thermal polymerisation followed by hydrothermal treatment and thermal exfoliation. Structural and morphological analyses indicate the preservation of the characteristic carbon nitride framework accompanied by partial delamination and increased exposure of layered domains. Electrochemical measurements revealed a concentration-dependent interfacial response, with 2 mg GCN ex providing the optimum performance. At this loading, the charge-transfer resistance for zinc corrosion increased from 1.891 to 8.080 Ω, corresponding to a corrosion inhibition efficiency of 76.60%, while the corrosion current density decreased from 0.480 to 0.274 mA cm⁻ 2 . Furthermore, HER measurements using Pt/C as a model HER-active electrode showed that GCN ex modification inhibited alkaline HER, increasing the onset potential from 38 to 152 mV, the overpotential at 10 mA cm −2 from 115 to 311, and increasing the apparent Tafel slope from 38.67 to 99.00 mV dec −1 . In a rechargeable ZAB operated at 5 mA cm⁻ 2 , the optimised electrolyte reduced the final charge–discharge voltage gap from 0.663 to 0.347 V after 24 h of cycling and increased the final-cycle areal operating power density from 4.98 to 5.81 mW cm⁻ 2 . Post-electrochemical SEM further revealed substantially reduced zinc surface degradation in the GCN ex -modified electrolyte.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Cyanide‐Driven Nitrite Trapping Enables Robustly‐Coupled Gel/Cathode Interfaces in Zinc‐Air BatteriesAdvanced Functional Materials · 2026
- Boosting zinc-air battery performance through interface-engineered N-C/g-C3N4 photoelectric synergy.Journal of colloid and interface science · 2026
- Synergistic interface engineering of FeNi-LDH/N-doped carbon hybrids for an ultra-low bifunctional voltage gap in zinc-air batteries.Nanoscale · 2026
- Synergistically Modified CNF/PAM Hydrogel with LiCl and Carboxylated Graphene for Zinc-Air Batteries.Polymers · 2026
- Engineering Advanced Electrocatalysts for Energy‐Saving Zinc−Air Hybrid Batteries: Concurrent Energy Storage Coupled With Chemical UpgradingAdvanced Energy Materials · 2026
- Unlocking durable Zn-air batteries via bio-derived interfacial protection.Chemical communications (Cambridge, England) · 2026