Diode area melting of Ti6Al4V: effects of multi-laser processing on microstructure and residual stress.
Anqi Liang, Sarath Veetil, Kristian Groom, Kamran Mumtaz
School of Mechanical, Aerospace, and Civil Engineering, University of Sheffield, S1 3JD Sheffield, UK.
Key points
From the paper's conclusion- The effects of laser number and scanning speed (100, 150, 200, and 250 mm/min) on surface roughness, melt pool geometry, microstructure, simulated cooling rate, and residual stress were systematically investigated.
Abstract
Laser Powder Bed Fusion (LPBF) is a widely adopted additive manufacturing technique for producing geometrically complex metallic components. While this process yields fine microstructures that are beneficial for strength, the associated rapid thermal cycles generate steep temperature gradients and high residual stresses, which may lead to warping, cracking, and dimensional instability. Diode Area Melting (DAM) employs arrays of low-power diode lasers operating at a wavelength of 808 nm. The diode beams are integrated into a customised optical head that traverses the powder bed in the X-Y plane, enabling a broader thermal interaction area and reducing local cooling rate. In this study, single-layer Ti6Al4V samples were processed by DAM using 3, 4, and 5 aligned 808 nm diode lasers, each operating at 5 W. The effects of laser number and scanning speed (100, 150, 200, and 250 mm/min) on surface roughness, melt pool geometry, microstructure, simulated cooling rate, and residual stress were systematically investigated. DAM produced lower simulated cooling rates (2211-8400 K/s) than those typically reported for LPBF (10⁴-10⁷ K/s), leading to coarser HCP lath spacings (0.8-1.3 μm) and evidence of retained β. Near-surface tensile residual stresses of up to 138.2 MPa were measured. The simulated lower cooling rates and reduced residual stress indicate that DAM may provide improved control over solidification behaviour and stress evolution.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- In-situ Dynamic laser area heating during diode point melting for thermal gradient reduction in laser powder bed fusionMaterials & Design · 2025
- Effect of process parameters on surface integrity in laser powder bed fusion of Ti-6Al-4V alloyScientific Reports · 2025
- Effects of Laser Process Parameters on Melt Pool Thermodynamics, Surface Morphology and Residual Stress of Laser Powder Bed-Fused TiAl-Based CompositesMetals · 2025
- Effect of layer thickness on the microstructure and machinability of AlSi7Mg processed by laser powder bed fusionCIRP journal of manufacturing science and technology · 2025
- Thermal and elasto-plastic simulations of dual-laser powder bed fusion and comparative study of various scan strategiesEngineering with Computers · 2026
- Defect-tolerant and site-specific heterogeneity engineering in laser powder bed fusion metallic alloysFrontiers in Mechanical Engineering · 2026