From the paper's conclusion- This study analyzes the tensile properties and cracking mechanisms of semi-solid cast AlSi7Mg alloys with varying iron content: primary (Fe = 0.08%), recycled (Fe = 0.19%), and recycled high iron (Fe = 0.42%), produced via the Rheometal™ method.
Abstract
Abstract To enhance the sustainability of aluminum castings, the use of recycled alloys is increasing due to their lower energy demand and reduced carbon footprint. At the same time, semisolid metal (SSM) rheocasting is emerging as a viable alternative to High Pressure Die Casting (HPDC), enabling the processing of low-silicon aluminum alloys. This reduces the need for critical raw materials, such as primary silicon, and allows casting at lower temperatures, further improving efficiency. However, contaminants typically present in recycled alloys, particularly iron, influence castability, defect formation, and mechanical performance, requiring further investigation. This study analyzes the tensile properties and cracking mechanisms of semi-solid cast AlSi7Mg alloys with varying iron content: primary (Fe = 0.08%), recycled (Fe = 0.19%), and recycled high iron (Fe = 0.42%), produced via the Rheometal™ method. Tensile testing was performed on as-cast and T6 samples. Statistical analysis was applied to evaluate variability and statistical significance of the results. The results show that recycled alloys have a higher defect density at an increased iron content, leading to lower elongation, reduced strength, and greater variability than in the primary alloy (recycled alloy Fe=0.19%: as-cast Rp 0.2 =113±8 MPa, R m =208±15 MPa, e f =4.13±0.95 %; T6 Rp 0.2 =240±17 MPa, R m =279±27 MPa, e f =1.40±0.20 %). The T6 treatment improved strength but reduced ductility due to defect enlargement and surface blistering caused by solubilization step, particularly pronounced in the recycled alloy with high-iron content. Scanning electron microscopy (SEM) fractography indicated that oxide films act as nucleation sites for β-Al 5 FeSi intermetallics, which promote shrinkage defects and thereby limit elongation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- From Recycled Aluminum to Automotive Material: A Through‐Process Adjustment Strategy for Mitigating the Negative Impacts of Fe‐Contained Intermetallic CompoundsAdvanced Sustainable Systems · 2026
- Heat Treatment Optimization of High-Pressure Die Casting Automotive Components Made in High Recycled AlSi10MnMg AlloyMetallurgical and Materials Transactions A · 2026
- Effect of Alloying Elements on the Intermetallic Phases and Mechanical Behaviour of Recycled Al-Si AlloysJournal of Physics: Conference Series · 2026
- Impurity-Tolerance Design and Strengthening–Toughening Strategies in Recycled Aluminium AlloysCrystals · 2026
- Mechanical and microstructural property assessment of recycled Al-alloys for automotive application: A sustainable engineering solutionJournal of Materials Research and Technology · 2026
- Innovative SolidStir extrusion for energy-efficient metal recyclingMaterials & Design · 2026