Decoding Hydrogen-Bond Network of Electrolyte for Cryogenic Durable Aqueous Zinc-Ion Batteries

Xiyan Wei, Jinpeng Guan, Yongbiao Mu, Yuhan Zou, Xianbin Wei, Lin Yang, Quanyan Man, C. Y. Yang, Limin Zang, Jingyu Sun, Lin Zeng

原始摘要(英文原文)· Original abstract
Abstract Aqueous zinc-ion batteries (AZIBs) hold great promise for next-generation energy storage but face challenges such as Zn dendrite growth, side reactions, and limited performance at low temperatures. Here, we propose an electrolyte design strategy that reconstructs the hydrogen-bond network through the synergistic effect of glycerol (GL) and methylsulfonamide (MSA), enabling the formation of a (100)-oriented Zn anode. This design significantly broadens the operating current and temperature windows of AZIBs. As a result, Zn||Zn symmetric cells exhibit remarkable cycling stability, achieving 4,000 h at 1 mA cm −2 and 600 h at 40 mA cm −2 (both at 1 mAh cm −2 capacity); even at −20 °C, Zn||Zn symmetric cells deliver ultra-stable cycling for over 5,400 h. Furthermore, Zn||VO 2 full cells retain 77.3% of their capacity after 2,000 cycles at 30 °C with a current density of 0.5 A g −1 and 85.4% capacity retention after 2,000 cycles at −20 °C and 0.25 A g −1 . These results demonstrate a robust pathway for enhancing the practicality and low-temperature adaptability of AZIBs.
读原文 · Read the paper ↗

AI 追问PRO

登录后使用 AI 追问

讨论区

登录后参与讨论

相关论文 · Related

Decoding Hydrogen-Bond Network of Electrolyte for Cryogenic Durable Aqueous Zinc-Ion Batteries — 科研速览 Science Skim