Hydrogen Embrittlement Analysis in Nitrogen and Vanadium Alloyed Supermartensitic Stainless Steels
Pedro S. P. Garcia, Marcos L. Augusto, Sérgio S. M. Tavares, André R. Pimenta, Juan Manuel Pardal
Key points
From the paper's conclusion- In this sense, this study investigated the susceptibility to hydrogen embrittlement of two distinct supermartensitic stainless steels, one containing nitrogen micro-additions and the other vanadium.
Abstract
Hydrogen embrittlement (HE) is a phenomenon for which numerous models have been proposed over the years to elucidate its underlying mechanisms. This poses a challenge for industry, especially for facilities and components in the oil country tubular goods (OCTG), as it compromises the structural integrity of metallic materials and can lead to catastrophic failures. In this sense, this study investigated the susceptibility to hydrogen embrittlement of two distinct supermartensitic stainless steels, one containing nitrogen micro-additions and the other vanadium. Both alloys underwent different heat treatments representing potential industrial solutions. To detect this phenomenon, slow strain rate tensile (SSRT) tests were conducted under cathodic polarization in an aqueous solution containing 3.5% NaCl. The resulting flow curves were modeled, and the adjusting parameters were compared. Fracture surface analyses were performed using scanning electron microscopy (SEM), enabling the qualitative characterization of failure mechanisms induced by the presence of hydrogen and their correlation with the obtained curves and parameters. The results showed a significant discrepancy between the alloy’s mechanical response to hydrogen charging and a considerable influence of the applied heat treatments. It became evident that microstructural changes, such as the presence of carbides and retained austenite, are directly correlated to embrittlement severity. Therefore, this study is a step forward in the development of safer and more resistant materials for applications in harsh environments within the oil and gas industry.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part II: Some Aspects of the Microstructural Mechanisms of Hydrogen-Assisted Damage and FractureMetals · 2026
- Region-resolved study of hydrogen embrittlement mitigation in CrMoV welds through post-weld heat treatmentInternational Journal of Hydrogen Energy · 2026
- Effect of Pre-Strain on Hydrogen Embrittlement Behavior of Metallic Materials: A Critical Review.Materials (Basel, Switzerland) · 2026
- Effects of sensitization on hydrogen embrittlement behavior in 304 stainless steelMaterials & Design · 2025
- Hydrogen embrittlement in pre-loaded sharply-notched samples of cold-drawn pearlitic steel wires for prestressed concrete structures: a fractographic analysisTheoretical and Applied Fracture Mechanics · 2026
- Hydrogen Embrittlement Resistance of an Austempered Martensite/Bainite Dual-Phase Steel.Materials (Basel, Switzerland) · 2026