From the paper's conclusion- We elucidate the structural evolution throughout the sonication duration (3, 5, 7, and 12 min) using Raman spectroscopy, x-ray diffraction (XRD), and scanning electron microscopy (SEM) under controlled thermal conditions.
Abstract
Abstract This work thoroughly investigates how different durations of ultrasonic treatment affect the structural, chemical, and morphological features of graphene oxide (GO) obtained from graphite through the Staudenmaier method. To ensure efficient exfoliation, a dual-source ultrasonic configuration (40 KHz, 100 W bottom transducer combined with a 100 W submerged probe) was utilized in pulse mode. We elucidate the structural evolution throughout the sonication duration (3, 5, 7, and 12 min) using Raman spectroscopy, x-ray diffraction (XRD), and scanning electron microscopy (SEM) under controlled thermal conditions. The initial GO, which underwent 3 min of sonication, had thick, stacked flakes bearing the markings of an XRD peak at 10.46° (0.845 nm d-spacing), suggesting the presence of highly oxidized and expanded layers evident from the peak intensity ratio ( I D / I G ) of 1.11. The structural evolution of GO during sonication resulted in significant reduction and rearrangement toward an optimum at 7 min, marked by a single dominant remaining reduced graphene oxide (rGO) XRD peak at 26.17° (0.340 nm d-spacing) and a decrease in I D / I G to 0.59, indicating substantial sp 2 lattice restoration and deoxygenation. This was accompanied by substantial structural restoration and deoxygenation. The 5-min mark provided morphological insight into the initial stage of exfoliation of GO, marked by thin, wrinkled sheets. However, prolonged treatment of 12 min led to an energy saturation effect, causing the I D / I G to increase to 0.72 and the dominant XRD peak to shift back toward larger d-spacing at 20.19° (0.439 nm). This suggests a reversal of structural benefits due to mechanical fragmentation and disordered restacking induced by excessive acoustic cavitation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fast Microwave-assisted synthesis of Reduced Graphene OxideJournal of Physics: Conference Series · 2026
- Graphite, graphene oxide, and reduced graphene oxide: comparative characterization of optical, morphological, structural and electric relaxation propertiesGreen Processing and Synthesis · 2026
- Tuning structural, optical, charge storage, and electronic transport properties of graphene oxide through functional group engineeringScientific Reports · 2026
- Optical properties analysis of a graphene oxide layer deposited between air and a dielectric substrateFrontiers in Physics · 2026
- From graphene oxide (GO) to reduced graphene oxide (rGO) films: A hybrid approach combining film transfer and vapor reduction for enhanced structural and optical propertiesCarbon Trends · 2026
- Synergistic Role of Electron and Photon Doses in Stepwise Laser-Induced Complete Deoxygenation of Graphene Oxide Revealed by In-Situ TEMThe Journal of Physical Chemistry C · 2026