Effect of CO2 laser irradiation on shear bond strength and enamel surface roughness after ceramic brackets removal: in vitro study.
Andira Mar-Ramírez, Laura Emma Rodríguez-Vilchis, Rogelio José Scougall-Vilchis, Motohiko Nagayama, Rosalía Contreras-Bulnes
Facultad de odontología, Centro de Investigación y Estudios Avanzados en Odontología, "Dr. Keisaburo Miyata" (CIEAO), Universidad Autónoma del Estado de México, Toluca, Mexico. · Facultad de odontología, Centro de Investigación y Estudios Avanzados en Odontología, "Dr. Keisaburo Miyata" (CIEAO), Universidad Autónoma del Estado de México, Toluca, Mexico. lerodriguezv@uaemex.mx.
Key points
From the paper's conclusion- This study aimed to evaluate the shear bond strength and surface roughness of the enamel after removal of ceramic brackets with CO2 laser.
Abstract
This study aimed to evaluate the shear bond strength and surface roughness of the enamel after removal of ceramic brackets with CO2 laser. Thirty extracted premolars were randomly assigned to three groups (n = 10): Untreated enamel (GI), Conventional debonding (GII), and CO2 laser debonding (GIII). Polycrystalline ceramic brackets were adhered on the buccal surface of GII and GIII groups, using 35% phosphoric acid and Transbond Plus Color Change resin (3 M Unitek; Monrovia, California, USA); shear bond strength was evaluated with a universal testing machine (EZ Graph; Shimadzu, Kyoto, Japan). Prior to debonding, brackets in the GIII group were irradiated with a CO2 laser (Yoshida Dental MFG; Tokyo, Japan) at a wavelength of 10.6 μm, power output of 6 W, for 5 s, at 5 mm. Each specimen was evaluated for adhesive remnant index score, and enamel surfaces were polished to assess roughness (with and without the CO2 laser) under atomic force microscopy. Ra, Rq, and Ry roughness parameters were analyzed. Statistical analysis was carried out using Student's t-test to evaluate shear bond strength, the Mann-Whitney U to assess the adhesive remnant index, and the Kruskal-Wallis and Dunn's post hoc to examine enamel roughness. GIII group showed statistically significant differences, with a reduction in shear bond strength (p < 0.001) and enamel roughness (p < 0.0083) compared to GII. These findings indicate that CO2 laser irradiation can be considered as an alternative in debonding ceramic brackets in orthodontic treatments.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of the CO2 laser on enamel surface roughness after debonding ceramic brackets and the application of nanohydroxyapatite: in-vitro study.Frontiers in dental medicine · 2026
- Morphometric analysis of enamel surface integrity after chemical, ultrasonic, and Er:YAG laser-assisted bracket debonding.Journal of orofacial orthopedics = Fortschritte der Kieferorthopadie : Organ/official journal Deutsche Gesellschaft fur Kieferorthopadie · 2026
- Effects of a cold atmospheric plasma device utilizing ambient air on bracket bonding to human enamel and surface roughness after debonding.Clinical oral investigations · 2026
- Shear bond strength of new and recycled orthodontic brackets to enamel surface: an in-vitro study.Frontiers in dental medicine · 2026
- Effect of Er: YAG laser on the bond strength of glass ceramic to bleached enamel and mechanism investigation.BMC oral health · 2026
- Er:YAG laser irradiation versus conventional surface treatments: a pull-out bond strength study on glass fiber posts.Lasers in medical science · 2026