Comparative screening of natural resins, gums and waxes as bio-based binders for lignocellulosic paper composites
Matthias Pfaff, Janina Sachtleben, Cordt Zollfrank
Key points
From the paper's conclusion- Overall, the results show a trade-off among reinforcement, moisture protection, and biodegradability, indicating that natural binders should be selected based on use-case requirements rather than as a universal replacement for synthetic binder systems.
Abstract
The properties of lignocellulosic composite materials are in general largely influenced by the binder used in their production. Binders ensure mechanical strength, extend the product’s lifespan, and significantly impact its environmental footprint. Traditional petrochemical-based binders are not sustainably sourced. Furthermore, they are often a major source of formaldehyde exposure and are mostly poorly biodegradable. Therefore, more environmentally friendly solutions are necessary. To serve as a viable replacement, a new binder system must achieve a balance between mechanical performance, moisture resistance, and environmental compatibility. This work focuses on selected natural waxes, resins, and gums, which are grouped under the term natural binders. In a screening approach, they were evaluated for their potential as bio-based binders for wood fiber composites in form of bound wood paper. Before utilization, the materials were characterized regarding their chemical composition, solubility for application, and thermal behavior. Binder-coated wood paper sheets were produced by solvent application and hot pressing, followed by tensile testing under standard conditions and after accelerated hygrothermal weathering. Moisture stability was assessed by water absorption measurements. Biodegradation was investigated under aerobic soil conditions via CO₂ evolution. All investigated natural binders improve the tensile strength and stiffness of the wood paper substrate compared with the unbound reference. Polysaccharide-rich gums show the strongest mechanical reinforcement. In contrast, waxes and several resin-based binders provide the highest water repellency. Biodegradation behavior also varies strongly with binder chemistry. Polysaccharide-rich gums exhibited the highest mineralization to CO 2 , with up to 77.4% after 91 days. Highly hydrophobic waxes and resins showed only limited degradation. Overall, the results show a trade-off among reinforcement, moisture protection, and biodegradability, indicating that natural binders should be selected based on use-case requirements rather than as a universal replacement for synthetic binder systems.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Wood Adhesives: Smart Adhesion, Aging, and Sustainability AssessmentACS Engineering Au · 2025
- Sustainable Bonding for the Built Environment: A Review on Bio-Based Adhesives and Their Multifunctional Synergistic Design.Polymers · 2026
- Bio-based adhesives from distillers’ dried grains and soybean for wood composites:review on performance and sustainabilityEuropean Journal of Wood and Wood Products · 2026
- Boron-based fire retardancy for natural polymeric materialsFrontiers in Chemistry · 2026
- Recent advances in bio-based adhesives: sustainable materials, synthesis strategies, and emerging applicationsJournal of Adhesion Science and Technology · 2025
- Engineering of particleboards using bio-based modified starch as a sustainable alternative to conventional bindersEuropean Journal of Wood and Wood Products · 2026