Kinetics and mechanisms of high-temperature oxidation of stainless steel 347LSi in synthetic air
Gleryston T. G. da Silva, Helen R. Araújo, André A. Vicente, Aureliano X. Santos, Renato A. C. de Santana, Edwar A. Torres-López, Tiago Felipe A. Santos
Key points
From the paper's conclusion- This study investigates the oxidation kinetics and mechanisms of coatings deposited by GMAW process on 2.25Cr–1Mo steel substrates, using different Ar–CO 2 shielding gas mixtures, in a synthetic air atmosphere at 800, 900, 1000, and 1100 °C.
Abstract
The high-temperature oxidation behavior of 347LSi stainless steel coatings is a critical factor for their application in aggressive environments. This study investigates the oxidation kinetics and mechanisms of coatings deposited by GMAW process on 2.25Cr–1Mo steel substrates, using different Ar–CO 2 shielding gas mixtures, in a synthetic air atmosphere at 800, 900, 1000, and 1100 °C. Thermogravimetric analysis revealed predominantly parabolic oxidation behavior for all conditions at times above 10 4 s, allowing the determination of parabolic rate constants (kₚ) and apparent activation energies (Eₐ). At 800 °C, the coatings exhibited low kₚ values and formed a compact and adherent bilayer oxide scale composed of an inner Cr 2 O 3 layer and an outer (Fe, Mn, Cr) 2 O 4 spinel, providing effective protection against oxidation. As the temperature increased to 900–1100 °C, a transition to accelerated oxidation was observed, associated with chromium depletion at the metal/oxide interface and the progressive breakdown of the protective chromia layer. This resulted in the formation of Fe-rich, porous, and poorly adherent oxides, promoting oxide spallation and loss of protective behavior. The shielding gas composition significantly influenced oxidation performance. The mixture containing 4% CO 2 exhibited the best overall behavior, combining lower oxidation rates with improved oxide stability, whereas higher CO 2 contents promoted faster degradation at elevated temperatures. These results demonstrate that oxidation resistance is maintained up to approximately 800 °C, while higher temperatures lead to a transition toward non-protective oxidation mechanisms. The findings highlight the critical role of shielding gas selection in controlling high-temperature oxidation and provide practical guidelines for the design of stainless steel coatings for demanding service conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Steam oxidation of 316Nb Stainless-Steel from 850°C to 1350°C: kinetics and thermodynamic analysisNuclear Materials and Energy · 2026
- Thermodynamic and kinetic analyses of high temperature oxidation of 316L stainless steelResults in Materials · 2025
- Microstructural Characterization and High-Temperature Oxidation Behavior of NiCrAlY/YSZ Coating on 20G SteelJournal of Manufacturing and Materials Processing · 2026
- Oxidation and degradation of Cr-coated Zr-based alloy up to 1500°C: Effect of Cr thicknessJournal of Nuclear Materials · 2026
- The effect of carbon and silicon variation on the oxidation resistance of a cobalt-based superalloyCorrosion Science · 2026
- Long-term stability and oxidation behavior of Mn2CuO4, Mn1.9Fe0.1CuO4, Mn1.7Fe0.3CuO4 coatings on SOFC interconnects: summary of a 10,000-h oxidation testJournal of Power Sources · 2026