Rupture and growth of holes in the melt pool during laser keyhole welding of thin sheets
Love O. John, Alexander F.H. Kaplan
Key points
From the paper's conclusion- This study investigates the formation and growth of holes during laser keyhole welding of 100 μm thin 316 L stainless-steel sheets in overlap joints, represented by bead-on-plate welding of 200 μm thick foils.
Abstract
This study investigates the formation and growth of holes during laser keyhole welding of 100 μm thin 316 L stainless-steel sheets in overlap joints, represented by bead-on-plate welding of 200 μm thick foils. Using high-speed imaging, keyhole instabilities, promoted by increasing line energy, were identified as precursors to hole nucleation. Continuous weld seams were obtained up to approximately 7 kJ/m, while hole formation occurred beyond this regime and cutting became dominant above approximately 12 kJ/m. The hole growth mechanism is described by the competition between vertical and horizontal surface-tension components associated with the local melt pool curvature. Once nucleated, holes expanded at approximately 0.8–1.2 m/s over 1–3 ms and developed into elliptical shapes before forming permanent perforations or cuts. A geometric stability criterion based on the Young-Laplace force balance indicates that unstable growth occurs when the hole length becomes comparable to the sheet thickness. The thinner the foil, the stronger the vertical force component promoting hole growth, reaching 17 kN/m² here. A systematic flow chart linking the observed sequence of keyhole instability, hole nucleation, and hole growth provides a basis for identifying precursor signatures and suppressing hole formation during thin-sheet laser welding.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fundamental mechanisms of spatter formation during full penetration laser welding revealed by high-speed synchrotron X-ray imagingWelding in the World · 2026
- Numerical and experimental study on spatter formation mechanisms and suppression method during ultra-high power laser-arc hybrid weldingJournal of Materials Processing Technology · 2025
- Tailoring sapphire–invar welds using burst femtosecond laserLight Advanced Manufacturing · 2025
- Numerical modelling of laser welding pool thermal-dynamics and dissimilar materials mixing of cast iron, carbon-steel and nickel-alloy wire for weld crack preventionJournal of Manufacturing Processes · 2025
- Investigation of the Cavitation Micro-Forming Mechanism and Forming Characteristic of 1060 Aluminum Foil Between Parallel Walls.Micromachines · 2026
- Synchrotron radiation imaging-based understanding of spatter reduction condition in laser beam keyhole welding of austenitic stainless steels through superimposed intensitiesOptics & Laser Technology · 2026