Enhancing spalling prevention of self‐compacting concrete at elevated temperatures: Incorporation of steel‐ PVA fibers
Liangli Xiao, Kaiyi Zhou, Liyuan Zhu, Zhao Yang
Key points
From the paper's conclusion- This study proposes a synergistic reinforcement scheme of steel and polyvinyl alcohol (PVA) fibers, with steel fiber volume fractions of 0, 0.4%, 0.8%, 1.2%, 1.4% and PVA fiber volume fractions of 0.1%, 0.2%, 0.3%.
Abstract
Self‐compacting concrete (SCC) is widely used for its excellent workability, but its dense internal structure causes spalling at elevated temperatures, which poses a critical risk to structural integrity and engineering safety. This study proposes a synergistic reinforcement scheme of steel and polyvinyl alcohol (PVA) fibers, with steel fiber volume fractions of 0, 0.4%, 0.8%, 1.2%, 1.4% and PVA fiber volume fractions of 0.1%, 0.2%, 0.3%. The effects of single‐doped and hybrid fibers on the high‐temperature spalling resistance of SCC were investigated via high‐temperature tests, gas permeability measurements, mercury intrusion porosimetry (MIP), and scanning electron microscopy (SEM). Results show that ≥0.1 vol.% PVA fibers completely prevent SCC spalling under engineering high‐temperature conditions, compared with 100% spalling of the reference group; 1.4% single‐doped steel fibers reduce the spalling degree to 4.32%, providing practical dosage references. SCC gas permeability remains acceptable below 400°C but degrades sharply above 600°C, and higher fiber content effectively retards this degradation to maintain steam‐release capacity. 400°C is the critical temperature for pore‐structure degradation, where thermal‐stress concentration accelerates interfacial microcracking and impairs structural performance. Microscopic analyses reveal that PVA fibers melt at ~230°C to form interconnected steam‐venting channels with slight pore coarsening, while steel fibers restrain crack propagation via three‐dimensional bridging for complementary interfacial protection. A temperature‐dependent two‐stage synergistic mechanism is proposed: steel fibers control cracks below 400°C, and PVA fibers realize steam‐pressure relief above 400°C. This greatly improves the high‐temperature spalling resistance of SCC and offers theoretical–experimental support for its fire‐resistant engineering design.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Compression behavior of steel‐ PVA high‐strength self‐compacting concrete short column exposed to elevated temperaturesStructural Concrete · 2026
- Effect of Polypropylene Fiber Content on the High-Temperature Performance of Steel Slag UHPS.Materials (Basel, Switzerland) · 2026
- Influence of fibers on the multiscale properties of fly ash and slag based geopolymer foam concreteConstruction and Building Materials · 2026
- Fibre-Reinforced Concrete at Elevated Temperatures: Damage Mechanisms, Spalling, and Residual Performance.Materials (Basel, Switzerland) · 2026
- Residual Flexural Behaviour of Reinforced Self-Compacting Concrete Beams After Fire Exposure: Effects of Fine-to-Coarse Aggregate Ratio, Heating Rate, and Boundary RestraintConstruction Materials · 2026
- Fractal Characteristics of Steel–Polypropylene Hybrid Fiber-Reinforced Concrete Under Impact LoadingCoatings · 2026