Weak-Solvation Reconstruction of PVDF-Based Quasi-Solid-State Electrolytes Enabling Potassium-Ion Batteries Working at -5°C.
Changzhang Jian, Maoting Xia, Yuanqian Huang, Zhihao Liang, Panpan Han, Juanjuan Cheng, Yun Ou, Dong Luo,
Hunan Provincial Key Laboratory of Advanced Materials For New Energy Storage and Conversion, School of Materials Science and Engineering, Hunan University of Science and Technology, Xiangtan, P. R. China. · School of Physics and Electronics, Hunan University, Changsha, P. R. China.
Key points
From the paper's conclusion- Furthermore, K|TSPE|PB batteries demonstrate 82.8% capacity retention over 600 cycles at room temperature and 90% retention after 180 cycles at -5°C, charting a viable trajectory for safe, long-life SSPIBs.
Abstract
Solid-state potassium-ion batteries (SSPIBs) promise next-generation energy storage with abundant resources, intrinsic safety, prolonged cycle life and broad operational temperature ranges. However, their practical application at room temperature is still severely restricted. Although poly(vinylidene fluoride) (PVDF)-based quasi-solid-state electrolytes (SPEs) can achieve room-temperature operation via residual polar solvents, these highly reactive solvents inevitably trigger severe interfacial parasitic reactions and detrimental polymer dehydrofluorination. To resolve this critical dilemma, we propose a "weak-solvation reconstruction" strategy by formulating PVDF-based SPEs with sterically hindered triethyl phosphate (TSPE). By improving ion transport and promoting the formation of inorganic interphases, this weak-solvation strategy effectively suppresses solvent-induced corrosion and polymer dehydrofluorination. The customized electrolyte delivers a high room-temperature ionic conductivity (7.22 × 10-4 S cm-1) and a K+ transference number of 0.58. Symmetric K|TSPE|K cells achieve stable plating/stripping exceeding 5500 h. Furthermore, K|TSPE|PB batteries demonstrate 82.8% capacity retention over 600 cycles at room temperature and 90% retention after 180 cycles at -5°C, charting a viable trajectory for safe, long-life SSPIBs.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Solvation engineering decouples bulk and interfacial chemistry for robust potassium-ion batteriesNature Communications · 2026
- Potassium-ion batteries for stationary energy storage solutions.Chemical Society reviews · 2026
- Key Materials for Potassium‐Ion Batteries: Overcoming Challenges and Opening Up Horizons for CommercializationAdvanced Materials · 2026
- Electrolyte Solvation Chemistry and Systemic Safety in Potassium‐Ion BatteriesSmall Structures · 2026
- Molecular Design of Crystalline Potassium Pyridonate Electrolytes for All-Solid-State Potassium Metal BatteriesJournal of the American Chemical Society · 2026
- Dead-Potassium Activation Reconstructing Stabilized Interface Enables Stable Anode-Free Potassium Metal Batteries.Journal of the American Chemical Society · 2026