Small (Weinheim an der Bergstrasse, Germany)

Tailoring Li/LATP Interface with In Situ Convertible ZrOP Layer for Solid-State Li Metal Batteries.

Jianfang Yang, Kaili Li, Hao Lai, Xianyong Zhang, Jinggu Huang, Pengfeng Jiang, Fangyan Xie, Xueyi Lu,

School of Materials, Sun Yat-sen University, Shenzhen, China. · Instrumental Analysis & Research Center, Sun Yat-sen University, Guangzhou, China.

Key points

From the paper's conclusion
  • A low-cost and scalable spray-coating strategy is used to construct an amorphous zirconium oxophosphate (ZrOP) interfacial layer on LATP.
  • The Li/ZrOP-LATP/Li symmetric cell achieves stable cycling for over 1300 h at 0.1 mA cm-2 with a critical current density of 2.1 mA cm-2, and the Li/ZrOP-LATP/LiFePO4 cell delivers a capacity retention of 82% after 480 cycles at 0.5C.
  • This work provides a facile and effective strategy to simultaneously resolve the chemical instability and poor physical contact at the Li/LATP interface, paving the way toward low-cost and high-performance SSLBs.

Abstract

NASICON-type Li1.3Al0.3Ti1.7(PO4)3 (LATP) has emerged as one of the most promising solid-state electrolytes owing to its high ionic conductivity, superior air stability, and low cost. However, the application of LATP-based solid-state lithium batteries (SSLBs) is hindered by its poor chemical compatibility with Li. Here, a low-cost and scalable spray-coating strategy is proposed to construct an amorphous zirconium oxophosphate (ZrOP) interfacial layer on LATP, which physically isolates LATP from Li to prevent the reduction of Ti4+ species and the formation of a mixed ionic and electronic conductivity layer. Moreover, the ZrOP layer undergoes an in situ reaction with Li, generating a nanocomposite mixture of Li-ion conductors, including LiZr2(PO4)3, Li2O, Li8ZrO6, and Li3P during cycling. This transformed interlayer maintains intimate contact to facilitate rapid Li-ion transport. Consequently, the Li/ZrOP-LATP/Li symmetric cell achieves stable cycling for over 1300 h at 0.1 mA cm-2 with a critical current density of 2.1 mA cm-2. The resultant Li/ZrOP-LATP/LiFePO4 cell delivers a capacity retention of 82% after 480 cycles at 0.5C. This work provides a facile and effective strategy to simultaneously resolve the chemical instability and poor physical contact at the Li/LATP interface, paving the way toward low-cost and high-performance SSLBs.

Read the paper

Discussion · 1

Science Skim's AI key points, plus readers' public thoughts

Science SkimAI key points
Pinned
  • A low-cost and scalable spray-coating strategy is used to construct an amorphous zirconium oxophosphate (ZrOP) interfacial layer on LATP.
  • The Li/ZrOP-LATP/Li symmetric cell achieves stable cycling for over 1300 h at 0.1 mA cm-2 with a critical current density of 2.1 mA cm-2, and the Li/ZrOP-LATP/LiFePO4 cell delivers a capacity retention of 82% after 480 cycles at 0.5C.
  • This work provides a facile and effective strategy to simultaneously resolve the chemical instability and poor physical contact at the Li/LATP interface, paving the way toward low-cost and high-performance SSLBs.