Expansion‑Pressure‑Based Early Detection and Relative Severity Assessment of Lithium Plating in Prismatic LiFePO4/Graphite Batteries.
Qing Xiong, Caitong Yue, Zechen Wei, Tianyu Gu, Hanyu Hu, Xiaoxiao Zhao, Li Wang, Shengchang Ji,
School of Electrical Engineering and Automation, Hefei University of Technology, Hefei, China. · State Grid Ningbo Electric Power Supply Company, Ningbo, China.
Key points
From the paper's conclusion- Here, we investigate expansion pressure response of 32 Ah prismatic LiFePO4/graphite cells under various charging conditions and introduce a differential metric, dP/dQ (pressure change per unit capacity), to amplify the mechanical footprint of plating.
Abstract
Low-temperature and high-rate charging imposes limitations on graphite anodes, driving local potentials below 0 V vs. Li/Li+ and triggering lithium plating, which accelerates capacity fade and compromises safety. Conventional voltage monitoring is insensitive to the mechanical signatures of lithium deposition. Here, we investigate expansion pressure response of 32 Ah prismatic LiFePO4/graphite cells under various charging conditions and introduce a differential metric, dP/dQ (pressure change per unit capacity), to amplify the mechanical footprint of plating. Results show that dP/dQ surges sharply during the late stage of low-temperature charging, far above the ambient-temperature baseline, enabling identification of graphite-anode plating onset. We establish a detection threshold based on the maximum dP/dQ during normal intercalation and propose a temperature-compensated variant to minimize false alarms under varying operating temperatures. To evaluate graphite-anode plating severity, cells with controlled plating degrees are prepared via low-temperature cycling; five peak-shape features extracted from pressure curves exhibit monotonic trends with capacity loss, providing indicators for relative severity assessment. Plated cells show gradual capacity recovery over subsequent cycles, revealing a reversible window for timely intervention before irreversible loss dominates. This mechanical-sensing framework offers a practical, non-invasive approach for relative plating severity assessment under controlled single-cell conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Decoupling Electrolyte Degradation Pathways With Diverse Li Plating Processes on Graphite ElectrodesAdvanced Energy Materials · 2026
- Operando Quantifying Li Plating Processes in Lithium-Ion Pouch Cells.Angewandte Chemie (International ed. in English) · 2026
- Lithium Plating: Mechanism, Influencing Factors, and Detection MethodsBatteries & Supercaps · 2026
- Lithium-Ion Battery Safety Evaluation by Quantifying Lithium Plating Degree Based on Pressure Signals.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026
- Quantitative Diagnosis of Li Plating Morphology by Analyzing Response of Electrochemical Impedance Spectroscopy in Working Li BatteriesJournal of the American Chemical Society · 2026
- Depth-to-Areal Staging Heterogeneity Preceding Lithium Plating in Graphite Anodes Revealed by Operando Imaging.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026