Correlative Operando X-Ray Imaging and Diffraction Revealing Mechanical Failure Pathways in Lithium Metal Sulfide-Based All-Solid-State Batteries.
Linfeng Xu, James Le Houx, Tristan Manchester, Jinsong Zhang, Robin Norbert Wullich, Victor Alexander Gomez, Johannes Ihli, Sarbajit Banerjee,
PSI Center for Energy and Environmental Sciences, PSI, Villigen, Switzerland. · ISIS Neutron and Muon Source, Rutherford Appleton Laboratory, Didcot, UK.
Key points
From the paper's conclusion- A multimodal operando characterization approach combining X-ray computed tomography (XCT), X-ray diffraction (XRD), and stack pressure monitoring was used to elucidate degradation mechanisms in LiNi0.8Co0.1Mn0.1O2 (NCM811) | Li6PS5Cl (LPSC) | Li cells.
- Operando XCT and XRD measurements reveal reversible ∼6% volume changes in NCM811 particles during (de-)lithiation, and spatially resolved XRD uncovers heterogeneous lithiation and depth-dependent electrochemical activity across the cathode.
- This multimodal operando framework provides critical insights into degradation pathways and design principles for mechanically robust sulfide-based ASSBs.
Abstract
All-solid-state batteries (ASSBs) employing sulfide solid electrolytes and lithium metal anodes offer a promising route toward high energy density and improved safety. However, their practical implementation is hindered by coupled electro-chemo-mechanical interfacial instabilities, which evolve across multiple length scales and remain poorly understood under operating conditions. Here, we present a multimodal operando characterization approach combining X-ray computed tomography (XCT), X-ray diffraction (XRD), and stack pressure monitoring to elucidate degradation mechanisms in LiNi0.8Co0.1Mn0.1O2 (NCM811) | Li6PS5Cl (LPSC) | Li cells. By correlating particle-level morphology with lattice-scale structural and strain evolution, this approach provides a unified multiscale description of interfacial degradation. Simultaneous operando XCT and XRD measurements reveal reversible ∼6% volume changes in NCM811 particles during (de-)lithiation, while spatially resolved XRD uncovers heterogeneous lithiation and depth-dependent electrochemical activity across the cathode. Partial relaxation of interfacial microstrain is linked to oxidative decomposition of LPSC. At the LPSC|Li interface, operando XCT visualizes crack formation, lithium infiltration, and progressive contact loss caused by plating-induced stress, ultimately leading to mechanical disconnection and short-circuiting at higher current densities. These mechanically induced degradation processes are partially reversible during lithium stripping. This multimodal operando framework provides critical insights into degradation pathways and design principles for mechanically robust sulfide-based ASSBs.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- A multimodal operando characterization approach combining X-ray computed tomography (XCT), X-ray diffraction (XRD), and stack pressure monitoring was used to elucidate degradation mechanisms in LiNi0.8Co0.1Mn0.1O2 (NCM811) | Li6PS5Cl (LPSC) | Li cells.
- Operando XCT and XRD measurements reveal reversible ∼6% volume changes in NCM811 particles during (de-)lithiation, and spatially resolved XRD uncovers heterogeneous lithiation and depth-dependent electrochemical activity across the cathode.
- This multimodal operando framework provides critical insights into degradation pathways and design principles for mechanically robust sulfide-based ASSBs.
Readers' thoughts
No reader thoughts yet.
Related papers
- Operando X‐Ray Computed Tomography Reveals the Role of Interfacial Nucleation Nanolayers in Suppressing Mechanical Failure in Zero‐Excess Lithium All‐Solid‐State BatteriesSmall · 2026
- Electro-Chemo-Mechanical Coupling in All-Solid-State Lithium Metal Batteries: From Stress Generation to Failure MitigationBatteries · 2026
- Interfacial chemistry-driven reaction dynamics and resultant microstructural evolution in lithium-based all-solid-state batteriesNature Communications · 2025
- NCM811–Sulfide Electrolyte Interfacial Degradation Mechanisms and Regulation Strategies in All‐Solid‐State Lithium BatteryChemSusChem · 2025
- Operando Imaging of Whisker Growth in NASICON Solid-State Batteries.Nano letters · 2026
- Visualizing a Li-Depleted Amorphous Cathode-Electrolyte Interphase in Sulfide Solid-State Batteries Using In Situ Cryogenic Electron Microscopy.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026