Morphological Stabilization of CsPbBr3 Quantum Dot Films Enabled by PVC-g-PMMA Graft Copolymer Encapsulation for Water-Robust Color Conversion.
Seung Ryeol Song, Kyungwon Seo, Uoon Chul Baek, Min-Gon Shin, Chanwung Mun, Hyosung An, Jung Tae Park
Department of Integrated Display Engineering, Yonsei University, Seoul, Republic of Korea. · Department of Petrochemical Materials Engineering, Chonnam National University, Yeosu-si, Jeollanam-do, Republic of Korea.
Key points
From the paper's conclusion- Herein, water-stable CsPbBr3 quantum dot-polymer composite films are prepared from a morphology-stabilizing copolymer, poly(vinyl chloride)-graft-poly(methyl methacrylate) (PVC-g-PMMA), where PMMA provides carbonyl-mediated passivation of CsPbBr3 defects and confers solvent compatibility and PVC endows water and chemical resistance.
Abstract
All-inorganic CsPbBr3 perovskite quantum dots are color-conversion emitters for display and lighting applications because of their high color purity and solution-processability. However, their application remains limited by poor water stability and photoluminescence (PL) degradation. Herein, water-stable CsPbBr3 quantum dot-polymer composite films are prepared from a morphology-stabilizing copolymer, poly(vinyl chloride)-graft-poly(methyl methacrylate) (PVC-g-PMMA), where PMMA provides carbonyl-mediated passivation of CsPbBr3 defects and confers solvent compatibility and PVC endows water and chemical resistance. CsPbBr3 and CsPbBr3/PVC-g-PMMA achieve PL quantum yields of 16.32% and 50.64%, respectively. In water, PL intensity of CsPbBr3/PVC-g-PMMA is >60% of its initial intensity after 28 days, whereas that of CsPbBr3/PMMA is <20% after 7 days. Upon UV irradiation and water exposure, CsPbBr3/PVC-g-PMMA maintains >70% after 12 h. Upon ethanol exposure, CsPbBr3/PVC-g-PMMA and CsPbBr3/PMMA retain >90% and <10%, respectively, after 4 h. Time-dependent ex situ transmission electron microscopy with particle segmentation reveals suppressed particle coalescence and preserved particle-size uniformity. The coefficient of variation of the maximum Feret diameter remains ∼0.25-0.27 for CsPbBr3/PVC-g-PMMA but increases to 0.81 for CsPbBr3/PMMA and CsPbBr3. Leave-one-out cross-validation indicates that this coefficient explains PL-intensity variations. In situ liquid atomic force microscopy reveals persistent regions with relatively high apparent local stiffness under hydration, indicating mechanical constraint.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Connecting the Dots: Excitation-Driven Self-Cross-Linking of CsPbBr3 Quantum Dots Enables Bright, Highly Transparent, and Stable Films.Nano letters · 2026
- Incorporation of CsPbBr3 quantum dot into polymer fibers via low-polarity co-solvent electrospinning.RSC advances · 2026
- In Situ Encapsulation of High‐Efficiency CsPbBr₃ Quantum Dots in Silica Aerogel for Ultra‐Stable Luminescence in Aqueous and High‐Temperature EnvironmentsAdvanced Optical Materials · 2026
- Water‐Resistant Polymer Films of Cyan‐Emitting CsPbBr 2.1 Cl 0.9 Perovskite Nanocrystals for Underwater Wireless Optical CommunicationLaser & Photonics Reviews · 2026
- Dual-Solvent Screening for Nondestructive In-Situ Optical Patterning of CsPbX3 QDs/PMMAACS Energy Letters · 2026