Influence of Fiber Orientation and Laminate Architecture on the Mechanical, Thermal, and Morphological Performance of Rattan Fiber/Epoxy Composites
Gogan Dhar, M. S. Rabbi, Md. Mahmudul Adil, Md. Abdul Hasib, Afnan Hasan
Key points
From the paper's conclusion- To investigate the impact of fiber orientation and stacking sequence on the characterization of rattan fiber epoxy composites, eight laminates with fiber orientations and stacking sequences of [0°] 4 , [30°] 4 , [60°] 4 , [90°] 4 , [0°/90°] 2 , [0°/90°] s , [±45°] 2 , and [0°/30°/60°/90°] were fabricated using vacuum bagging method.
Abstract
To investigate the impact of fiber orientation and stacking sequence on the characterization of rattan fiber epoxy composites, eight laminates with fiber orientations and stacking sequences of [0°] 4 , [30°] 4 , [60°] 4 , [90°] 4 , [0°/90°] 2 , [0°/90°] s , [±45°] 2 , and [0°/30°/60°/90°] were fabricated using vacuum bagging method. Mechanical properties, including tensile, flexural, and rockwell hardness; thermal properties, including thermogravimetric and differential scanning calorimetry analysis; Fourier Transform Infrared Spectroscopy; and morphological characteristics were evaluated in this study. The [0°] 4 laminate demonstrated the maximum tensile strength of 18.43 MPa and Young's modulus of 2.77 GPa, while the [90°] 4 laminate demonstrated the lowest tensile strength of 4.87 MPa, indicating that load transmission is strongly dependent on fiber alignment. With a strength of 34.99 MPa, [0°] 4 had the best flexural performance, while the symmetric [0°/90°] s laminate had the greatest flexural modulus of 3.75 GPa, closely followed by [0°] 4 laminate (3.73 GPa). Hardness test results were almost constant between 66–68 HRL, suggesting that fiber orientation had minimal impact. Thermogravimetric analysis revealed multi‐stage degradation, with maximum decomposition temperatures between 370°C–380°C and significant weight loss (40%–55%) taking place between 350°C‐450°C. Glass transition temperatures were found to be between 87°C–89°C using differential scanning calorimetry. Cellulose, lignin, and epoxy functional groups were confirmed by FTIR, while SEM evaluation showed reasonable fiber–matrix wetting along with voids, interfacial debonding, fiber pull‐out, and fiber splitting in all laminates. Finally, the experimental findings of both Young's modulus and flexural modulus were compared with theoretical predictions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Advancement in rattan fiber reinforced composites: Surface treatment, fabrication, characterization, hybridization, and industrial applicationJournal of Reinforced Plastics and Composites · 2026
- Architecture-Specific Performance of Silica and MWCNT Modified Hybrid Epoxy Laminates Under Mechanical Loading and Fracture.Polymers · 2026
- Sustainable Epoxy Composites Reinforced With Date Palm and Palmyra Palm Fibers: Mechanical and Thermal CharacterizationSPE Polymers · 2026
- Chemical and structural characterization of ramie-based epoxy composites reinforced with macadamia nut shell biocharScientific Reports · 2026
- Vacuum Heat Treatment Regulates the Bamboo-Epoxy Interface: Balancing Mechanical Performance and Thermal Stability.Polymers · 2026
- Effects of Curing Schedules on Carbon-Fiber-Reinforced Laminates with a Bio-Based Epoxy Matrix.Polymers · 2026