Modified bismaleimide with benzoxazine containing tert ‐butyl group: preparation, characterization and properties
Yiqing Xia, Zhenggang Zhou, Yuping Sheng, Shuai Yan, Chunguang Zhu, Wilfred Emori, Renfei Zhang, Chenghong Fu,
Key points
From the paper's conclusion- These results confirm that introducing the tert ‐butyl group effectively improves the dielectric properties, thermal stability and moisture resistance of benzoxazine‐modified BMI systems, suggesting that these copolymers are promising low‐dielectric thermoset candidates. © 2026 Society of Chemical Industry.
Abstract
With the rapid development of high‐frequency communication and electronic integrated circuits, high thermal performance and low dielectric resin have become active research areas in recent years. In this paper, four benzoxazines (Bz, Bz‐o, Bz‐p, Bz‐m) were synthesized by Mannich reaction of trimethylhexanediamine, paraformaldehyde and different phenols (phenol, o ‐ tert ‐butylphenol, m ‐ tert ‐butylphenol and p ‐ tert ‐butylphenol). The chemical structure and curing behavior of the benzoxazine monomers were characterized using Fourier transform infrared and 1 H NMR spectroscopies and differential scanning calorimetry, and the results showed that four benzoxazine resins were successfully synthesized. And then, these benzoxazines were used to modify bismaleimide resin (BMI‐70) by copolymerization, and the effects of introduction of the tert ‐butyl group and its substitution position on properties were explored. The results demonstrated that incorporating the low‐polarity, bulky tert ‐butyl group reduced the polarizability of the copolymers and increased their free volume, thereby improving their dielectric properties. The dielectric constant ( D k ) of the copolymer decreased from 3.09 to 2.87 at 10 MHz, while the dissipation factor ( D f ) ranged from 0.0024 to 0.0041 at 10 MHz. Water absorption was also markedly reduced: the tert ‐butyl‐containing copolymers absorbed 2.06–2.47% water, compared with 3.02% for P(BMI/Bz). Among these prepared copolymers, the para ‐substituted tert ‐butyl variant exhibited the most balanced overall performance, with a glass transition temperature of 298 °C, D k of 2.88, D f of 0.0026, water absorption of 2.43% and CY of 33.4% at 800 °C. These results confirm that introducing the tert ‐butyl group effectively improves the dielectric properties, thermal stability and moisture resistance of benzoxazine‐modified BMI systems, suggesting that these copolymers are promising low‐dielectric thermoset candidates. © 2026 Society of Chemical Industry.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Synthesis of Monofunctional Benzoxazine Resin Containing Acetylamino Group and Properties of Its Copolymer With Epoxy ResinPolymers for Advanced Technologies · 2026
- Synthesis, Characterization and Dielectric Properties of Biphenyl Group Containing Polymaleimide and Cyanate Ester CopolymerJournal of Applied Polymer Science · 2026
- Synthesis of Monofunctional Benzoxazines Containing Trifluoroacetylamino and Furanyl Groups and Their Thermal, Dielectric, and Adhesive Properties in Copolymers with Epoxy ResinsACS Applied Engineering Materials · 2026
- Complementary Hydrogen-Bonded Dual-Network Bismaleimides for Cohesive Adhesion at Metal–Polymer InterfacesACS Applied Polymer Materials · 2026
- A Minireview of Benzoxazine-Based Photopolymer Resins for Vat Photopolymerization: Recent Progress and Future Perspectives Toward Low-Dielectric Applications.Macromolecular rapid communications · 2026
- Economical bisphenol-based dibenzocyclobutene resins with excellent thermal and dielectric properties for high-frequency communication applications.RSC advances · 2026