Key points
From the paper's conclusion- The laminate flexural strength decreased from 942 to 844 MPa, corresponding to 89.6% retention, which was notably higher than that of the matched carbon fiber‐reinforced epoxy control (81.5%) under identical exposure conditions.
Abstract
The resin matrices used in fiber‐reinforced polymer composites for marine infrastructure and coastal engineering are required to possess exceptional durability. This study investigated the accelerated exposure response of the melamine‐hexamethylenediamine (MH) thermoset and carbon fiber‐reinforced MH laminates. After 60 days, the measured mass increases of MH resin were 1.56, 1.36, and 1.22 wt.% in simulated seawater sea sand concrete (SWSSC) pore solution, NaCl solution, and deionized water, respectively. After 120 days in SWSSC pore solution at 60°C, the resin tensile strength decreased from 74 to 69 MPa, corresponding to approximately 93.2% retention. The laminate flexural strength decreased from 942 to 844 MPa, corresponding to 89.6% retention, which was notably higher than that of the matched carbon fiber‐reinforced epoxy control (81.5%) under identical exposure conditions. Surface observations revealed increased roughness and localized damage. Fourier transform infrared spectroscopy showed no evidence of new functional groups, and thermogravimetric analysis revealed only marginal changes in the thermal decomposition behavior, suggesting that no extensive bulk degradation occurred. Gel permeation chromatography of the dimethyl sulfoxide‐soluble fraction showed a molecular weight decrease after prolonged exposure, indicating chain scission of soluble products, though no extensive bulk degradation occurred. Molecular dynamics simulations further indicate that the weak hydrogen‐bonding affinity between water molecules and the cross‐linked network, together with the low free volume of the MH network, may reduce the driving force for water adsorption and wetting and hinder water penetration.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Durability of Marine‐Service Carbon‐Fiber‐Reinforced Polymer Composites: Scenario‐Resolved Moisture Transport, Multiscale Damage, and Engineering ImplicationsPolymer Composites · 2026
- Durability of Polyurethane Based CFRP Bars Used for Mooring Cables Under Marine Environments: A Combined Experimental and Molecular Dynamics StudyPolymer Composites · 2026
- Long-term flexural performance and microstructural evolution of 3D-printed carbon, glass, and aramid fibre-reinforced polymer under hygrothermal exposureConstruction and Building Materials · 2025
- Study of Hybrid Epoxy Resin Composites Reinforced with E-CR Glass Fiber/Polypropylene: Moisture Behavior, Mechanical Strength, and Acoustic Damage Mitigation Under Marine Aging Conditions.Polymers · 2026
- Moisture Uptake, Mechanical Degradation, and Long‐Term Performance Prediction of MXene ‐Modified BFRP Laminates Under Alkaline ExposurePolymer Composites · 2026
- The Effect of Silicone Modification on the Thermo-Oxidative Degradation and Mechanical Property Retention of CFRP Laminates.Polymers · 2026