Effect of Carbon Fiber, Graphene Nanoplatelet, and Chain‐Extender Reinforcement on the Hygrothermal Durability of 3D ‐Printed PLA Composites: A Combined Mechanical and Thermal Study
Nevin Gamze Karsli, Taner Yilmaz, Sinan Fidan, Mehmet İskender Özsoy, Satılmış Ürgün, Mustafa Özgür Bora
Key points
From the paper's conclusion- Hygrothermal durability of FDM printed polylactic acid (PLA) composites containing short carbon fiber (CF, 3 wt%), graphene nanoplatelets (GnP, 0.5 wt%), and epoxy‐functional chain extender (Joncryl, 0.1 wt%) was studied.
Abstract
Hygrothermal durability of FDM printed polylactic acid (PLA) composites containing short carbon fiber (CF, 3 wt%), graphene nanoplatelets (GnP, 0.5 wt%), and epoxy‐functional chain extender (Joncryl, 0.1 wt%) was studied. Printed filaments obtained using two‐step extrusion were exposed to up to 400 freeze‐heat cycles from −20°C to +40°C at 93% relative humidity and further analyzed through gravimetric, tensile, DSC, and SEM studies. Whereas the GnP additive caused the maximum moisture uptake of 0.336%, the uncompatibilized hybrid of CF and GnP demonstrated a non‐monotonic behavior (moisture uptake reached 0.400% at 200 cycles, but dropped to 0.143% at 400 cycles) with temporary loss of mechanical performance and presence of interphase cavities (image analysis: 51 cavities mm −2 , 19.9% area fraction, equivalent diameter up to 127 μm). Incorporation of Joncryl prevented any increase of moisture uptake (0.179%), avoided any loss of strength during aging, maintained ductility, and produced the highest strength (51.48 MPa) and stiffness (4173.3 MPa) after 400 cycles. Factorial ANOVA showed formulation to be the main factor (about 50% of the variance for strength and 61% for modulus), with a secondary, non‐monotonic effect of aging; the formulation × aging interaction was not statistically significant. Within the investigated formulations and exposure conditions, the Joncryl‐modified composite was the most hygrothermally stable.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Long-term flexural performance and microstructural evolution of 3D-printed carbon, glass, and aramid fibre-reinforced polymer under hygrothermal exposureConstruction and Building Materials · 2025
- Fracture Behavior of Natural Fiber‐Reinforced PLA/TPU Hybrid Composites Produced by Material Extrusion Additive ManufacturingFatigue & Fracture of Engineering Materials & Structures · 2026
- Mechanical performance and failure analysis of additively manufactured PLA–carbon fibre, PLA–glass fibre, ABS–carbon fibre, and ABS–glass fibre compositesInternational Polymer Processing · 2026
- Impact of hot water aging on the mechanical performance and shape memory behavior of 4D-printed flax fiber-reinforced PLA/PETG compositesComposites Part B Engineering · 2026
- Polylactic Acid Hybrid Composites Reinforced with Thermally Modified Wood Flour and Cellulose NanofibrilsApplied Sciences · 2026
- Effect of Hygrothermal Aging on the Tensile Performance of GNP‐Modified Patch‐Repaired GFRP CompositesPolymer Composites · 2026