Polymer Composites

Beyond β‐Phase Fraction: Structure–Property Relationships in Corona‐Poled Poly(Vinylidene Fluoride)/Titanium Dioxide Nanocomposite Films

Ibtisam Yahya Abdullah

Key points

From the paper's conclusion
  • Because film thickness increased with TiO 2 loading, the piezoelectric results are interpreted as composition‐dependent structure–property relationships under the employed processing and film‐thickness conditions.

Abstract

Poly(vinylidene fluoride) (PVDF)/titanium dioxide (TiO 2 ) composite films were fabricated by solution casting from N,N‐dimethylformamide (DMF) with TiO 2 loadings of 0, 1, 5, 10, and 15 wt%. Scanning electron microscopy (SEM), x‐ray diffraction (XRD), Fourier‐transform infrared spectroscopy (FTIR), and d 33 measurements were carried out to study the effect of TiO 2 loading in terms of morphology, crystalline structure, electroactive fraction of the β‐phase, and piezoelectric response. The β‐phase fraction increased from 79.88% for pristine PVDF to 90.27% at 15 wt% TiO 2 . In contrast, the highest measured d 33 was 34 ± 1.70 pC/N at 10 wt% TiO 2 , compared with 20 ± 1.00 pC/N for pristine PVDF. At this composition, the XRD‐derived relative crystallinity reached 74%, and the FWHM decreased to 1.98°. At 15 wt% TiO 2 , the d 33 decreased to 30 ± 1.50 pC/N despite the higher β‐phase fraction, accompanied by lower crystallinity and greater morphological heterogeneity. Because film thickness increased with TiO 2 loading, the piezoelectric results are interpreted as composition‐dependent structure–property relationships under the employed processing and film‐thickness conditions.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers